#Login Register
RH Testing Lighweight Concrete
  • 0 Vote(s) - 0 Average


09-21-2009, 05:59 AM #1
JDJR Newbie *
Status: Offline Posts:5 Threads:2 Joined:Sep 2009
What are the procedures for testing Lightweight Concrete, and can you get a true reading.

09-22-2009, 03:42 PM #2
Ben Newbie *
Status: Offline Posts:5 Threads:1 Joined:Sep 2008
ASTM F2170. I don't see why you wouldn't get a true reading when following that method.

09-24-2009, 04:10 PM #3
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
What is the thickness of lightweight concrete? Anyone know? Smile

09-28-2009, 05:24 AM #4
JDJR Newbie *
Status: Offline Posts:5 Threads:2 Joined:Sep 2009
The thickness is 6"

12-16-2009, 12:05 PM #5
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Lightweight is scary! The aggregate is very porous and as such holds a great amount of water. Drying time for lightweight concrete can be 300% longer than standard concrete. I'd figure 3 months per inch of thickness and go from there.

I had a job that was on 11" of lightweight and I had MVER readings of 3lbs - 4lbs, with RH readings of 96%. The floor failed after the first year (that's when I was called in) and we ended up coating the floor with a Moisture Mitigation System.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 14,415 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 37,417 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 45,037 Views
Last Post by eaadams
11-08-2013, 01:41 PM
2 Replies 12,080 Views
Last Post by eaadams
09-27-2013, 10:26 AM
35 Replies 116,911 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 17,300 Views
Last Post by eaadams
01-30-2013, 04:43 PM
33 Replies 95,208 Views
Last Post by eaadams
11-21-2012, 10:19 AM
51 Replies 159,615 Views
Last Post by ILLENTINC
11-19-2012, 11:59 AM
4 Replies 17,905 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
22 Replies 63,034 Views
Last Post by Ernesto
07-30-2012, 07:01 PM

Users browsing this thread:
1 Guest(s)