11-20-2012, 05:45 PM #31
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
I think I would have opted for a nicely color stained, sealed concrete surface. Granted they would have long term maintenance issues with waxing and re-sealing every couple of years or so, but it would have been breathable until the end of time.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

11-20-2012, 05:49 PM #32
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Maybe a polished and hardened floor?

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

11-20-2012, 05:54 PM #33
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
...another viable option for sure

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

11-21-2012, 10:19 AM #34
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
oh... static disipating, heat welded ... well there are few manufacturers of those. Most are private labeled coppies








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 15,876 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
4 Replies 16,340 Views
Last Post by CC Solutions
12-20-2013, 10:23 PM
2 Replies 13,042 Views
Last Post by eaadams
09-27-2013, 10:26 AM
21 Replies 88,765 Views
Last Post by CCR
07-19-2013, 05:14 PM
51 Replies 171,256 Views
Last Post by ILLENTINC
11-19-2012, 11:59 AM
4 Replies 19,252 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
22 Replies 67,611 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
62 Replies 175,129 Views
Last Post by CC Solutions
12-07-2011, 07:27 AM
36 Replies 124,739 Views
Last Post by CC Solutions
04-19-2011, 04:59 PM
9 Replies 37,054 Views
Last Post by CC Solutions
04-05-2011, 05:33 AM

Users browsing this thread:
1 Guest(s)