CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Perhaps you misunderstand my position on carbide testing....

It is a soils test being spec'd by silicate pushers because they think they can fool people into believing it means something.

The way they are testing means nothing to anyone in the flooring industry.

As for CaCl testing, it is nearly worthless for determining the potential a floor has for failure. I'd rather put in 5 Wagners at a cost of $200 (including installation and reading) than 7 CaCl tests for the same cost, when the CaCl tests tell you nothing about the condition of the slab, and the results are unreliable.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Carbide moisture testing - CC Solutions - 09-18-2012, 10:19 AM
RE: Carbide moisture testing - eaadams - 09-18-2012, 11:01 AM
RE: Carbide moisture testing - CC Solutions - 09-18-2012, 12:25 PM
RE: Carbide moisture testing - eaadams - 09-18-2012, 02:02 PM
RE: Carbide moisture testing - CC Solutions - 09-18-2012, 06:11 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 10,660 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
4 Replies 13,991 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 36,054 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 8,968 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 11,814 Views
Last Post by eaadams
09-27-2013, 10:26 AM
33 Replies 93,320 Views
Last Post by eaadams
11-21-2012, 10:19 AM
51 Replies 156,391 Views
Last Post by ILLENTINC
11-19-2012, 11:59 AM
22 Replies 61,830 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
23 Replies 83,049 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 19,407 Views
Last Post by Ernesto
08-14-2011, 08:43 PM

Users browsing this thread:
1 Guest(s)