Calcium Carbide testing and Silicates
  • 0 Vote(s) - 0 Average


09-24-2012, 10:51 AM #20
Newenglandci Newbie *
Status: Offline Posts:2 Threads:0 Joined:Sep 2012
Hello Mr. Lepito, I am the first inspector/testing agent on that job. I am surprised to find that has not been taken care of by now. Researching the carbide testing turned up nothing on my end either other than it's use in Europe. My next step was to locate the ASTM for it but found only one for soil using the carbide testing. My question was the same as to contamination as 1870 says concrete must be cleaned with no contaminants. The other side of the whole problem is the company, to my knowledge, has not said why the Lino blew off. Ambient does not cut it. My apologies for the syntax, or lack of, this is off my iPhone.








Messages In This Thread
Calcium Carbide testing and Silicates - Lepito - 09-15-2012, 08:12 AM
RE: Calcium Carbide testing and Silicates - eaadams - 09-15-2012, 09:04 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-15-2012, 11:38 AM
RE: Calcium Carbide testing and Silicates - eaadams - 09-15-2012, 12:32 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-15-2012, 02:00 PM
RE: Calcium Carbide testing and Silicates - Lepito - 09-15-2012, 06:13 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 09-16-2012, 06:34 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-16-2012, 09:15 PM
RE: Calcium Carbide testing and Silicates - eaadams - 09-16-2012, 10:50 PM
RE: Calcium Carbide testing and Silicates - Lepito - 09-17-2012, 07:38 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-18-2012, 07:47 AM
RE: Calcium Carbide testing and Silicates - Concrete1421 - 09-18-2012, 12:40 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-18-2012, 06:03 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 09-18-2012, 10:58 PM
RE: Calcium Carbide testing and Silicates - Lepito - 09-19-2012, 06:40 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-19-2012, 06:59 AM
RE: Calcium Carbide testing and Silicates - Lepito - 09-19-2012, 07:01 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-20-2012, 05:41 AM
RE: Calcium Carbide testing and Silicates - eaadams - 09-24-2012, 10:00 AM
RE: Calcium Carbide testing and Silicates - Newenglandci - 09-24-2012, 10:51 AM
RE: Calcium Carbide testing and Silicates - Newenglandci - 09-24-2012, 02:12 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-24-2012, 03:59 PM
RE: Calcium Carbide testing and Silicates - Specsystems - 09-27-2012, 10:41 AM
RE: Calcium Carbide testing and Silicates - eaadams - 10-15-2012, 03:47 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 10-15-2012, 03:54 PM
RE: Calcium Carbide testing and Silicates - eaadams - 10-15-2012, 04:38 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 10-15-2012, 06:12 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 10-15-2012, 08:04 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 10-15-2012, 08:34 PM
RE: Calcium Carbide testing and Silicates - Ernesto - 10-16-2012, 01:59 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 10-21-2012, 04:34 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-15-2012, 10:47 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-15-2012, 12:49 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-15-2012, 02:13 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-15-2012, 02:27 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-15-2012, 02:37 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 11-16-2012, 01:52 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 07:03 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-16-2012, 07:08 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 07:59 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-16-2012, 09:03 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 09:19 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-16-2012, 09:27 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 01:54 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-16-2012, 03:06 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 11:10 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-17-2012, 06:22 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-18-2012, 08:41 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-19-2012, 08:33 AM
RE: Calcium Carbide testing and Silicates - eaadams - 11-19-2012, 11:36 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-19-2012, 11:56 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-19-2012, 11:59 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 12,285 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
2 Replies 10,744 Views
Last Post by eaadams
09-27-2013, 10:26 AM
33 Replies 85,166 Views
Last Post by eaadams
11-21-2012, 10:19 AM
4 Replies 16,081 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
22 Replies 56,599 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
36 Replies 104,763 Views
Last Post by CC Solutions
04-19-2011, 04:59 PM
9 Replies 31,758 Views
Last Post by CC Solutions
04-05-2011, 05:33 AM
2 Replies 12,713 Views
Last Post by eaadams
09-30-2010, 08:27 AM
11 Replies 39,002 Views
Last Post by CC Solutions
09-20-2010, 03:01 PM
11 Replies 39,449 Views
Last Post by CC Solutions
05-11-2010, 03:22 PM

Users browsing this thread:
1 Guest(s)