09-24-2012, 02:12 PM #21
Newenglandci Newbie *
Status: Offline Posts:2 Threads:0 Joined:Sep 2012
Sorry. 1869

09-24-2012, 03:59 PM #22
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
(09-24-2012, 02:12 PM)Newenglandci Wrote:  Sorry. 1869

The silicate advocates can't test with 1869 because that test shows the floor still emits high levels of vapor. They are trying to come up with a test they can use that shows the concrete is suitable for flooring, but the tests they have proposed are flawed for many different reasons.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

09-27-2012, 10:41 AM #23
Specsystems Newbie *
Status: Offline Posts:1 Threads:0 Joined:Sep 2012
my opinion:
Calcium carbide testing is only as good as the opperator. For example if the "concrete" that is removed and pulverized for testing is really a piece of Rock that has little or no water in it the test will show very low. Calcium carbide works well for "self drying" screeds and self leveling cements that can not be accurately tested by other methods

10-15-2012, 03:47 PM #24
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
On Thursday 8/18/2012 in the morning there is a free breakfast seminar with Howard Kanare of CTL Group on concrete moisture and I am told it will have a new special section on silicates. (ASTM C309 discussion included)

It is in Northern California by SFO Airport.

AIA credits are available to those who qualify.

For those lurkers out there, PM me for an invite (but you'd have to join the forum to PM me! Tongue ).

10-15-2012, 03:54 PM #25
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
(10-15-2012, 03:47 PM)eaadams Wrote:  On Thursday 8/18/2012 in the morning there is a free breakfast seminar with Howard Kanare of CTL Group on concrete moisture and I am told it will have a new special section on silicates. (ASTM C309 discussion included)

It is in Northern California by SFO Airport.

AIA credits are available to those who qualify.

For those lurkers out there, PM me for an invite (but you'd have to join the forum to PM me! Tongue ).


I can't make it because my time machine is on the fritz... Unless you mean October 18th, then I can't make it because I'm tearing apart a hospital in northern WI. Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

10-15-2012, 04:38 PM #26
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
hand to forehead... doh. Frantically checked my e-mail invites.. breaths sigh of relief. 10/18/2012 @ 7:30AM

10-15-2012, 06:12 PM #27
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
I hope you can give us a brief update after you attend. Howard is great to listen to, and his new silicate findings are hopefully going to help me out. I haven't seen his latest report on silicate admixes and topicals but I hear it is due out soon or was just released.

Wish I could be there!!!!! Blush

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

10-15-2012, 08:04 PM #28
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
(10-15-2012, 03:54 PM)CC Solutions Wrote:  I can't make it because my time machine is on the fritz... Unless you mean October 18th,

Cheese goes well with fritz.

I wonder if all the silicate people from Linkedin are going to be at the seminar.. Big Grin

I am equally curious as to the findings. Certain silica based treatments are starting to take off down here. Not quite sure how to deal with them.

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher


10-15-2012, 08:34 PM #29
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Hopefully Howard's latest report debunks the silicate myth.....

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

10-16-2012, 01:59 PM #30
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Should I bring wading boots? Big Grin

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 16,871 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
2 Replies 13,666 Views
Last Post by eaadams
09-27-2013, 10:26 AM
33 Replies 107,702 Views
Last Post by eaadams
11-21-2012, 10:19 AM
4 Replies 20,210 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
22 Replies 70,712 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
36 Replies 129,937 Views
Last Post by CC Solutions
04-19-2011, 04:59 PM
9 Replies 38,494 Views
Last Post by CC Solutions
04-05-2011, 05:33 AM
2 Replies 14,826 Views
Last Post by eaadams
09-30-2010, 08:27 AM
11 Replies 46,274 Views
Last Post by CC Solutions
09-20-2010, 03:01 PM
11 Replies 48,631 Views
Last Post by CC Solutions
05-11-2010, 03:22 PM

Users browsing this thread:
1 Guest(s)