#Login Register
RH Testing For Parking Garages
  • 0 Vote(s) - 0 Average


07-12-2012, 07:56 AM #1
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Can anyone share any experience in performing RH tests in these exterior "unacclimated" environments? Concrete over steel decking precisely.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
RH Testing For Parking Garages - CCR - 07-12-2012, 07:56 AM
RE: RH Testing For Parking Garages - CC Solutions - 07-12-2012, 08:12 AM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 08:48 AM
RE: RH Testing For Parking Garages - CC Solutions - 07-12-2012, 09:00 AM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 09:14 AM
RE: RH Testing For Parking Garages - eaadams - 07-12-2012, 01:22 PM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 01:44 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 9,146 Views
Last Post by jim decker
07-13-2015, 02:51 PM
3 Replies 12,758 Views
Last Post by CC Solutions
09-01-2013, 09:10 AM
3 Replies 11,611 Views
Last Post by eaadams
06-28-2013, 10:26 AM
27 Replies 55,069 Views
Last Post by jim decker
05-02-2013, 12:31 PM
23 Replies 45,741 Views
Last Post by CCR
03-21-2013, 05:05 PM
23 Replies 66,711 Views
Last Post by CC Solutions
07-26-2012, 06:19 AM
1 Replies 8,703 Views
Last Post by hnelson
06-07-2012, 01:08 PM

Users browsing this thread:
1 Guest(s)