Can anyone share any experience in performing RH tests in these exterior "unacclimated" environments? Concrete over steel decking precisely.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

07-12-2012, 08:12 AM #2
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Hopefully your climate is stable and not fluctuating wildly.... Temperature is a factor of rH!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

07-12-2012, 08:48 AM #3
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Well, it's Pittsburgh, what can I say except temp at testing time was my first concern too. But this is no place to do Calcium Chloride tests. I would anticipate performing tests in the late spring thru early fall about the same time and ambient conditions the coating systems are to be applied. So technically, they would be conducted in conditions the manufacturer would recognize as acclimated (for application anyway). Other than that, I can think of nothing else to be concerned with off the top of my head.

I'm writing "blindly" right now because I have not read the manufacturer's literature yet. That's next

Always something new to consider, right?

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

07-12-2012, 09:00 AM #4
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
I would ask the manufacturer for their requirements first. If the coating is quite breathable they may be rather lax in their demands.

Typically though almost any finish requires some degree of dryness be inherent in the substrate. You wouldn't put ceramic tile on a 2 day old slab, but 30 days may be fine.

Determining the dryness is rather easy if the slab reaches a temperature conducive for testing. If the concrete never falls below 90 degrees, the rH can read quite low, yet the moisture present could be rather high. Likewise in the winter a cold slab would read artificially low. This is why we test at a standard expected temperature. Outside that range is going to be very wide spread, but you may get a good idea of comparable rH if you can read the slab around 70 degrees.

If the temperature is moving quickly, you may need to insure your probe and the sensor are acclimated also. Can you shade the area you are reading?

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

07-12-2012, 09:14 AM #5
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Appreciate your inputExclamation It appears all their coating systems call for CaCl testing. I can see it now...prep the test area, etc. per ASTM, place the kits and come to find a virtual rain forest inside the plastic cover and pellets solidified into a slimy, solid mass. Big Grin

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

07-12-2012, 01:22 PM #6
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
A lot of manufacturers if you call them have unpublished RH limits.

07-12-2012, 01:44 PM #7
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
True. I will definitely inquire on that.

Thanks.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 13,597 Views
Last Post by jim decker
07-13-2015, 02:51 PM
3 Replies 15,292 Views
Last Post by CC Solutions
09-01-2013, 09:10 AM
3 Replies 13,945 Views
Last Post by eaadams
06-28-2013, 10:26 AM
27 Replies 66,797 Views
Last Post by jim decker
05-02-2013, 12:31 PM
23 Replies 54,860 Views
Last Post by CCR
03-21-2013, 05:05 PM
23 Replies 77,869 Views
Last Post by CC Solutions
07-26-2012, 06:19 AM
1 Replies 9,860 Views
Last Post by hnelson
06-07-2012, 01:08 PM

Users browsing this thread:
1 Guest(s)