Hi All:

Could someone let me know if there is a test time restriction for the moisture testing using the RH probes? ASTM 2170 says that the RH and temperature reading should be taken after 72 hrs. Unlike the Calcium Chloride test, the insitu moisture test standard does not specify a not to exceed time for taking the readings. Does it make a difference if the reading is taken at say 84 hrs or 96 hrs given that the environment inside the building shell remains relatively the same during that time.

Thanks in advance for helping me get a solution to my question.








Messages In This Thread
Test time for RH test - jigar0896 - 09-01-2009, 09:38 PM
RE: Test time for RH test - Joe Greenberg - 09-03-2009, 04:03 PM
RE: Test time for RH test - Blake McFee - 09-04-2009, 08:51 AM
RE: Test time for RH test - RCConcrete Consulting - 09-21-2009, 05:13 PM
RE: Test time for RH test - CC Solutions - 12-17-2009, 11:01 AM
RE: Test time for RH test - RCConcrete Consulting - 12-17-2009, 01:12 PM
RE: Test time for RH test - CC Solutions - 12-18-2009, 09:53 AM
RE: Test time for RH test - RCConcrete Consulting - 12-18-2009, 03:37 PM
RE: Test time for RH test - CC Solutions - 12-28-2009, 08:09 AM
RE: Test time for RH test - Ernesto - 01-08-2010, 10:29 AM
RE: Test time for RH test - CC Solutions - 01-08-2010, 01:30 PM
RE: Test time for RH test - Ernesto - 01-12-2010, 09:40 AM
RE: Test time for RH test - CC Solutions - 01-13-2010, 07:14 AM
RE: Test time for RH test - Ernesto - 01-13-2010, 11:27 AM
RE: Test time for RH test - CC Solutions - 01-15-2010, 09:36 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
6 Replies 16,294 Views
Last Post by Ernesto
05-13-2013, 04:51 PM
10 Replies 27,574 Views
Last Post by eaadams
01-18-2013, 04:48 PM
16 Replies 45,596 Views
Last Post by CC Solutions
08-08-2011, 11:41 AM
3 Replies 15,615 Views
Last Post by Ernesto
08-30-2010, 12:42 PM
5 Replies 18,941 Views
Last Post by Ernesto
07-12-2010, 07:00 PM
2 Replies 11,877 Views
Last Post by eaadams
07-09-2010, 09:45 AM
2 Replies 12,516 Views
Last Post by CC Solutions
12-16-2009, 11:45 AM
1 Replies 12,920 Views
Last Post by EWagner
07-09-2009, 01:46 PM

Users browsing this thread:
1 Guest(s)