I believe you are right, as the prior version of 2170 did list an 'or' statement.

What we have found is the temperature will affect the readings, so we try to measure the concrete at the service temperature.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-12-2012, 07:26 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-12-2012, 01:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-19-2012, 12:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-19-2012, 07:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 03:18 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 03:50 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 07-24-2012, 04:37 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 05:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 05:46 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 06:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 08:25 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-25-2012, 10:14 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 10:28 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 01:44 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-26-2012, 02:33 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 02:49 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 07:27 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 09:38 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 10:46 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 02:34 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 03:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-16-2012, 09:23 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 06:01 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 07:16 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 07:50 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 10:30 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 10:51 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-19-2012, 04:11 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 16,297 Views
Last Post by CC Solutions
02-05-2011, 10:08 AM

Users browsing this thread:
1 Guest(s)