#Login Register
We're almost at 3lbs MVER, so what if the rH is over 90% ?
  • 0 Vote(s) - 0 Average


08-16-2012, 10:46 AM #19
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
(07-26-2012, 02:49 PM)Ernesto Wrote:  Huh

ASTM F-2170-11

9. Conditioning
9.1 Concrete floor slabs shall be at service temperature and the occupied air space above the floor slab shall be at service temperature and service relative humidity for at least 48 h before making relative humidity measurements in the concrete slab.

As you posted ^^^

You do not need a heater or a blower or a cooling system to provide the required conditions. Many facilities are within the stated parameters well before the HVAC system is functional.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-12-2012, 07:26 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-12-2012, 01:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-19-2012, 12:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-19-2012, 07:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 03:18 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 03:50 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 07-24-2012, 04:37 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 05:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 05:46 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 06:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 08:25 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-25-2012, 10:14 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 10:28 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 01:44 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-26-2012, 02:33 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 02:49 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 07:27 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 09:38 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 10:46 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 02:34 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 03:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-16-2012, 09:23 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 06:01 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 07:16 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 07:50 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 10:30 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 10:51 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-19-2012, 04:11 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 14,728 Views
Last Post by CC Solutions
02-05-2011, 10:08 AM

Users browsing this thread:
2 Guest(s)