We're almost at 3lbs MVER, so what if the rH is over 90% ?
  • 0 Vote(s) - 0 Average


08-16-2012, 09:38 AM #18
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
(07-26-2012, 02:33 PM)CC Solutions Wrote:  The HVAC does not have to be running for validity.

You cannot interpret the ASTM's as you feel they should be. The old MVER test never required grinding and never required HVAC. The new 2170 doesn't require HVAC.

If the temp is 70 and the humidity is 50, HVAC does nothing for you.

I'm still waiting for an explanation. If what you say is true about the HVAC running for validity, then why is it not in my 2170-11 standard? Is there an updated one I am not aware of?

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-12-2012, 07:26 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-12-2012, 01:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-19-2012, 12:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-19-2012, 07:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 03:18 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 03:50 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 07-24-2012, 04:37 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 05:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 05:46 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 06:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 08:25 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-25-2012, 10:14 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 10:28 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 01:44 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-26-2012, 02:33 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 02:49 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 07:27 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 09:38 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 10:46 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 02:34 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 03:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-16-2012, 09:23 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 06:01 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 07:16 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 07:50 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 10:30 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 10:51 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-19-2012, 04:11 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 16,296 Views
Last Post by CC Solutions
02-05-2011, 10:08 AM

Users browsing this thread:
1 Guest(s)