We're almost at 3lbs MVER, so what if the rH is over 90% ?
  • 0 Vote(s) - 0 Average


07-26-2012, 07:27 PM #17
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
(07-26-2012, 02:33 PM)CC Solutions Wrote:  The HVAC does not have to be running for validity.

You cannot interpret the ASTM's as you feel they should be. The old MVER test never required grinding and never required HVAC. The new 2170 doesn't require HVAC.

If the temp is 70 and the humidity is 50, HVAC does nothing for you.

Well, did you actually read the new ASTM or are your making that up?

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-12-2012, 07:26 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-12-2012, 01:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-19-2012, 12:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-19-2012, 07:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 03:18 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 03:50 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 07-24-2012, 04:37 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 05:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 05:46 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 06:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 08:25 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-25-2012, 10:14 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 10:28 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 01:44 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-26-2012, 02:33 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 02:49 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 07:27 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 09:38 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 10:46 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 02:34 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 03:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-16-2012, 09:23 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 06:01 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 07:16 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 07:50 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 10:30 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 10:51 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-19-2012, 04:11 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 16,314 Views
Last Post by CC Solutions
02-05-2011, 10:08 AM

Users browsing this thread:
1 Guest(s)