Status: Offline Posts:606 Threads:33 Joined:Sep 2009
(07-24-2012, 05:46 PM)CC Solutions Wrote:  I never contradict myself. Ever. Wink

I stand by the comment that I have not seen a properly conducted CaCl test.

Then how can you claim CaCL if performed properly is not a valid test? Oh, gotcha.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-12-2012, 07:26 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-12-2012, 01:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-19-2012, 12:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-19-2012, 07:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 03:18 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 03:50 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 07-24-2012, 04:37 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 05:40 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-24-2012, 05:46 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-24-2012, 06:04 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 08:25 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - eaadams - 07-25-2012, 10:14 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-25-2012, 10:28 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 01:44 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 07-26-2012, 02:33 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 02:49 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 07-26-2012, 07:27 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 09:38 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 10:46 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-16-2012, 02:34 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-16-2012, 03:25 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-16-2012, 09:23 PM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 06:01 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 07:16 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 07:50 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Ernesto - 08-17-2012, 10:30 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - CC Solutions - 08-17-2012, 10:51 AM
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ? - Rubensgt40 - 08-19-2012, 04:11 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 14,691 Views
Last Post by CC Solutions
02-05-2011, 10:08 AM

Users browsing this thread:
1 Guest(s)