Yea we don't accept CaCl tests anymore. Even people with a P.E. after their name seem to not be able to do it correctly. These pictures done by one of the more respected "professional building testing labs" in California.

Here is an example of this.
[Image: IMG_1475.JPG]




side note: oy the cracks Sad Lumpy Bumpy Slab will probably break poor church's budget. We want to fix the crack with Roadware Concrete Mender but at over $5 lft it is so expensive.

[Image: IMG_1477.JPG]








Messages In This Thread
RH & CC Testing - CCR - 07-10-2012, 10:35 AM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 06:37 AM
RE: RH & CC Testing - CCR - 07-12-2012, 07:25 AM
RE: RH & CC Testing - eaadams - 07-12-2012, 01:31 PM
RE: RH & CC Testing - CCR - 07-12-2012, 01:38 PM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 01:48 PM
RE: RH & CC Testing - JLG - 07-17-2012, 11:13 AM
RE: RH & CC Testing - CCR - 07-17-2012, 11:37 AM
RE: RH & CC Testing - Erica - 07-17-2012, 12:10 PM
RE: RH & CC Testing - CCR - 07-17-2012, 12:27 PM
RE: RH & CC Testing - eaadams - 07-18-2012, 11:19 AM
RE: RH & CC Testing - CCR - 07-18-2012, 11:32 AM
RE: RH & CC Testing - CC Solutions - 07-19-2012, 07:49 PM
RE: RH & CC Testing - CCR - 07-22-2012, 04:55 AM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 09:09 AM
RE: RH & CC Testing - CCR - 07-22-2012, 03:05 PM
RE: RH & CC Testing - Rubensgt40 - 07-22-2012, 07:19 PM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 07:33 PM
RE: RH & CC Testing - CCR - 07-24-2012, 04:07 PM
RE: RH & CC Testing - Rubensgt40 - 07-24-2012, 05:35 PM
RE: RH & CC Testing - CC Solutions - 07-24-2012, 05:49 PM
RE: RH & CC Testing - CCR - 07-25-2012, 03:49 AM
RE: RH & CC Testing - Rubensgt40 - 07-25-2012, 09:46 PM
RE: RH & CC Testing - CC Solutions - 07-26-2012, 06:19 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 11,227 Views
Last Post by jim decker
07-13-2015, 02:51 PM
3 Replies 14,010 Views
Last Post by CC Solutions
09-01-2013, 09:10 AM
3 Replies 12,819 Views
Last Post by eaadams
06-28-2013, 10:26 AM
27 Replies 61,320 Views
Last Post by jim decker
05-02-2013, 12:31 PM
23 Replies 50,392 Views
Last Post by CCR
03-21-2013, 05:05 PM
6 Replies 18,988 Views
Last Post by CCR
07-12-2012, 01:44 PM
1 Replies 9,330 Views
Last Post by hnelson
06-07-2012, 01:08 PM

Users browsing this thread:
1 Guest(s)