Blake,
About 40% the thickness of the slab. 4" slab about 1-1/2 - 1-3/4"
Rayt








Messages In This Thread
Moisture Meters - concreteworker27 - 09-11-2008, 09:00 AM
RE: Moisture Meters - rthompson - 09-12-2008, 01:28 PM
RE: Moisture Meters - Blake McFee - 09-12-2008, 05:42 PM
RE: Moisture Meters - rthompson - 09-15-2008, 04:19 PM
RE: Moisture Meters - rthompson - 10-21-2008, 11:49 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 9,408 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 31,057 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 7,962 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 10,743 Views
Last Post by eaadams
09-27-2013, 10:26 AM
4 Replies 16,081 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 77,147 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 17,933 Views
Last Post by Ernesto
08-14-2011, 08:43 PM
8 Replies 26,705 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
1 Guest(s)