#Login Register
Moisture Meters
  • 3 Vote(s) - 4.33 Average


09-11-2008, 09:00 AM #1
Blake McFee Newbie *
Status: Offline Posts:10 Threads:3 Joined:Sep 2008
I have heard that a surface moisture meter is not as good a way to measure moisture in concrete as using an internal relative humidity sensor. Could someone clarify this for me?

09-12-2008, 01:28 PM #2
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
Blake,
Correct, surface moisture meters and surface testing measures the very top of the concrete. As concrete dries from the top down, the slab may be wet at the bottom while indicating dry at the surface. Once a slab is covered with a moisture sensitive flooring the slab will go into equilibrium and the moisture will increase at the surface. The use of a RH Sensor will measure the internal moisture at the apex of the drying curve, which is the point where equilibrium crosses.
Please advise any questions
Rayt

09-12-2008, 05:42 PM #3
Blake McFee Newbie *
Status: Offline Posts:10 Threads:3 Joined:Sep 2008
Thanks, and how deep should I measure to get to the equilibrium point?

Blake

09-15-2008, 04:19 PM #4
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
ASTM F-2170 recommends 40% the thickness of the slab
Rayt

10-21-2008, 11:49 AM #5
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
Blake,
About 40% the thickness of the slab. 4" slab about 1-1/2 - 1-3/4"
Rayt








Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 10,674 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 36,104 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 8,977 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 11,826 Views
Last Post by eaadams
09-27-2013, 10:26 AM
4 Replies 17,559 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 83,080 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 19,413 Views
Last Post by Ernesto
08-14-2011, 08:43 PM
8 Replies 29,190 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
2 Guest(s)