Moisture Meters
  • 3 Vote(s) - 4.33 Average


09-11-2008, 09:00 AM #1
Blake McFee Newbie *
Status: Offline Posts:10 Threads:3 Joined:Sep 2008
I have heard that a surface moisture meter is not as good a way to measure moisture in concrete as using an internal relative humidity sensor. Could someone clarify this for me?

09-12-2008, 01:28 PM #2
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
Blake,
Correct, surface moisture meters and surface testing measures the very top of the concrete. As concrete dries from the top down, the slab may be wet at the bottom while indicating dry at the surface. Once a slab is covered with a moisture sensitive flooring the slab will go into equilibrium and the moisture will increase at the surface. The use of a RH Sensor will measure the internal moisture at the apex of the drying curve, which is the point where equilibrium crosses.
Please advise any questions
Rayt

09-12-2008, 05:42 PM #3
Blake McFee Newbie *
Status: Offline Posts:10 Threads:3 Joined:Sep 2008
Thanks, and how deep should I measure to get to the equilibrium point?

Blake

09-15-2008, 04:19 PM #4
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
ASTM F-2170 recommends 40% the thickness of the slab
Rayt

10-21-2008, 11:49 AM #5
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
Blake,
About 40% the thickness of the slab. 4" slab about 1-1/2 - 1-3/4"
Rayt








Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 8,615 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 28,248 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 7,351 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 10,094 Views
Last Post by eaadams
09-27-2013, 10:26 AM
4 Replies 15,167 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 73,881 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 17,135 Views
Last Post by Ernesto
08-14-2011, 08:43 PM
8 Replies 25,516 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
1 Guest(s)