Ardex should get away from that MVER statement soon. How can you measure MVER over an epoxy mitigation system? You can't follow the ASTM, that's for sure. Besides, who believes MVER readings anymore?

The only moisture suppression systems that I see applied to fresh concrete are the ones that use silicates. Like a Cure and Seal.

Since the big Koster shake up I have been putting down mostly Ardex MC and V1200. I bought a semi load last week in fact. It is a little learning curve for the crew, but they are coming around.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Mopped the Floor - eaadams - 06-25-2012, 01:44 PM
RE: Mopped the Floor - CC Solutions - 06-25-2012, 02:48 PM
RE: Mopped the Floor - eaadams - 06-28-2012, 04:47 PM
RE: Mopped the Floor - CCR - 07-02-2012, 10:57 AM
RE: Mopped the Floor - rapidrhrep - 07-02-2012, 12:35 PM
RE: Mopped the Floor - CC Solutions - 07-02-2012, 12:47 PM
RE: Mopped the Floor - eaadams - 07-09-2012, 01:30 PM
RE: Mopped the Floor - CCR - 07-10-2012, 11:47 AM
RE: Mopped the Floor - CC Solutions - 07-12-2012, 06:21 AM
RE: Mopped the Floor - eaadams - 07-12-2012, 01:09 PM
RE: Mopped the Floor - CC Solutions - 07-12-2012, 01:35 PM
RE: Mopped the Floor - eaadams - 07-18-2012, 11:15 AM
RE: Mopped the Floor - CC Solutions - 07-19-2012, 07:42 PM
RE: Mopped the Floor - CCR - 07-20-2012, 05:48 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 06:17 AM
RE: Mopped the Floor - CCR - 07-20-2012, 06:42 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 07:01 AM
RE: Mopped the Floor - CCR - 07-20-2012, 07:41 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 08:03 AM
RE: Mopped the Floor - CCR - 07-20-2012, 08:21 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 08:51 AM
RE: Mopped the Floor - rapidrhrep - 07-20-2012, 11:24 AM
RE: Mopped the Floor - CC Solutions - 07-20-2012, 11:53 AM

Users browsing this thread:
2 Guest(s)