I've got a deck that I've got to measure, and I hear that they dry differently, or that ASTM classifies them differently, or something along those lines, because it's up off the ground. Is that true?

07-09-2009, 01:46 PM #2
EWagner Administrator *******
Status: Offline Posts:50 Threads:19 Joined:Jul 2008
Is your concrete slab on a metal deck? How did you pour it?

Basically, ASTM F2170 says that if the slab is drying only from the top, you should drill to 40% into it for your test. If it's drying from both sides (which means it's not on a metal deck or sitting on the ground with a vapor retarder below) than you only should drill down 20% of the thickness








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 12,346 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 31,267 Views
Last Post by eaadams
05-19-2014, 10:55 AM
4 Replies 9,869 Views
Last Post by Ernesto
05-05-2014, 04:17 PM
16 Replies 47,560 Views
Last Post by Ernesto
04-15-2014, 02:30 PM
9 Replies 41,630 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 106,102 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 15,376 Views
Last Post by eaadams
01-30-2013, 04:43 PM
1 Replies 7,742 Views
Last Post by Rubensgt40
01-24-2013, 07:03 PM
32 Replies 96,364 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM

Users browsing this thread:
1 Guest(s)