#Login Register
How thick is your floor?
  • 0 Vote(s) - 0 Average


04-11-2012, 07:36 AM #18
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Not at all. At least not with slab on grade concrete. The testing protocol laid out in 2170 does a good job of exposing abnormalities, and any noted discrepancies can be further investigated by drilling confirming test holes for depth. So what I'm saying is if we install probes near exterior walls, near entrances and sprinkled throughout after that, and we know what the designed depth of the slab should be, a couple of proofing holes is all that would be required for a standard test. If probe readings start coming in all over the charts or if an installer wants to push the limits of a test, we may do more proofing.

Slabs in pans need to either use a floor scan tool or be drilled for depth to locate the flutes.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
How thick is your floor? - CC Solutions - 03-27-2012, 10:23 AM
RE: How thick is your floor? - eaadams - 03-27-2012, 01:14 PM
RE: How thick is your floor? - CC Solutions - 03-27-2012, 02:01 PM
RE: How thick is your floor? - Ernesto - 03-27-2012, 08:08 PM
RE: How thick is your floor? - CC Solutions - 03-28-2012, 06:06 AM
RE: How thick is your floor? - eaadams - 03-31-2012, 08:23 PM
RE: How thick is your floor? - Ernesto - 04-01-2012, 09:14 AM
RE: How thick is your floor? - CCR - 04-02-2012, 09:53 PM
RE: How thick is your floor? - eaadams - 04-03-2012, 09:56 AM
RE: How thick is your floor? - CC Solutions - 04-04-2012, 03:36 AM
RE: How thick is your floor? - Rubensgt40 - 04-10-2012, 06:14 PM
RE: How thick is your floor? - CC Solutions - 04-10-2012, 07:29 PM
RE: How thick is your floor? - Ernesto - 04-10-2012, 08:02 PM
RE: How thick is your floor? - CC Solutions - 04-10-2012, 08:16 PM
RE: How thick is your floor? - Ernesto - 04-10-2012, 08:41 PM
RE: How thick is your floor? - CC Solutions - 04-11-2012, 06:30 AM
RE: How thick is your floor? - Ernesto - 04-11-2012, 06:57 AM
RE: How thick is your floor? - CC Solutions - 04-11-2012, 07:36 AM
RE: How thick is your floor? - Taseera - 07-18-2013, 11:21 PM
RE: How thick is your floor? - CCR - 07-19-2013, 04:28 PM
RE: How thick is your floor? - CC Solutions - 07-19-2013, 04:38 PM
RE: How thick is your floor? - CCR - 07-19-2013, 05:14 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
35 Replies 100,509 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 14,395 Views
Last Post by eaadams
01-30-2013, 04:43 PM
33 Replies 80,591 Views
Last Post by eaadams
11-21-2012, 10:19 AM
2 Replies 12,841 Views
Last Post by eaadams
12-23-2011, 12:06 PM
46 Replies 137,306 Views
Last Post by CC Solutions
04-01-2011, 07:56 AM

Users browsing this thread: