JD - Please PM me a news link!! I want to know what company it was.

Just got off the phone with Ardex and they suggest I also consider K301 for indoor use under moisture systems (like Koester people use RapidSet) - unsure but I am going to run it by the boss.

Also Ardex recommended I closely check out Ardex MRP for patching / feathering under moisture systems. Will get a few bags to the guys to test out & play with.








Messages In This Thread
Ardex V1200 - CC Solutions - 03-27-2012, 09:57 AM
RE: Ardex V1200 - eaadams - 03-27-2012, 10:03 AM
RE: Ardex V1200 - CC Solutions - 03-27-2012, 10:36 AM
RE: Ardex V1200 - eaadams - 04-25-2012, 02:01 PM
RE: Ardex V1200 - CC Solutions - 04-25-2012, 04:06 PM
RE: Ardex V1200 - CCR - 04-26-2012, 04:36 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 06:11 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:11 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 07:18 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:33 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 07:16 PM
RE: Ardex V1200 - eaadams - 04-26-2012, 08:36 PM
RE: Ardex V1200 - CC Solutions - 04-27-2012, 06:06 AM
RE: Ardex V1200 - eaadams - 05-07-2012, 09:45 AM
RE: Ardex V1200 - CC Solutions - 05-07-2012, 12:27 PM
RE: Ardex V1200 - eaadams - 07-10-2012, 10:28 AM
RE: Ardex V1200 - CCR - 07-10-2012, 11:40 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 06:19 AM
RE: Ardex V1200 - CCR - 07-12-2012, 07:49 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 08:10 AM
RE: Ardex V1200 - eaadams - 07-12-2012, 12:56 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:33 PM
RE: Ardex V1200 - eaadams - 07-12-2012, 01:42 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:50 PM
RE: Ardex V1200 - CCR - 07-12-2012, 02:46 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 04:25 PM

Users browsing this thread:
2 Guest(s)