Hey,

Has anyone tried both the Rapid RH long reader and short reader? I know the short reader used to be the standard, but now it seems like Wagner is pushing the long one. Does any one have any preferences, or know why?

Thanks.

07-10-2009, 09:51 AM #2
EWagner Administrator *******
Status: Offline Posts:50 Threads:19 Joined:Jul 2008
From Wagner:
Quote:Wagner has found that many people prefer the standard (long) reader, simply because it's easier to hold on to. On the other hand, there are those who like to leave the reader in the hole and purchase the short reader.

08-26-2011, 03:15 PM #3
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
I prefer the long reader, I have fat fingers and it is difficult to use the short ones. I would see no value in leavng the short readers in the sensor. I would think someone might need them worse than you do!
Rayt

08-27-2011, 08:55 AM #4
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
I think the new orange long reader has the ability to hold the info after taken out of the hole. Besides the fact it's easier to use on deeper depths. I gots fat fingers as well.

What do you guys use for getting the short reader in and out of deeper holes?

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

08-27-2011, 12:44 PM #5
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
I used a loop of chalk line attached to the bail on the reader. I would keep it tight to allow me to hold the bail up so II could find the slot and turn into position.
Rayt

08-28-2011, 02:02 PM #6
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Back when we had the short reader I just drilled all holes an inch deep. That made it easy to use the reader.






NOT!!! Big Grin But hey, I did find some guys that actually wouldn't drill deeper than 1 1/2" because they couldn't get the reader in and out.... Seriously!


I have a small needle-nose pliers that worked pretty good. Love the longer reader though.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
19 Replies 61,965 Views
Last Post by CC Solutions
10-16-2011, 06:09 PM
4 Replies 14,933 Views
Last Post by CC Solutions
10-13-2011, 03:09 PM
10 Replies 33,580 Views
Last Post by CC Solutions
03-24-2011, 07:00 AM
11 Replies 37,797 Views
Last Post by CC Solutions
05-11-2010, 03:22 PM
7 Replies 26,617 Views
Last Post by CC Solutions
12-17-2009, 12:16 PM
1 Replies 10,732 Views
Last Post by rthompson
02-20-2009, 01:08 PM

Users browsing this thread:
1 Guest(s)