03-09-2012, 06:14 AM #8
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
I've found more often than not on a renovation project, no one knows, or will take the time to find records of slab depths, and you have to place the sensors NOW.

I keep a 12" length of coat hanger with a pre-formed hook at the end in my tool case. I trill a 3/8" hole all the way thru the slab (after determining there is now rebar there with my Bosch sensor), push the wire thru, pull up til the hook catches and you have your depth. Obviously slab depths can vary, so it's up to you and the GC or Flooring Installer how many areas you drill thru and it adds time to your testing costs. So, I just establish a cost per hole and let them make the call. Just make sure you document everything agreed to in your report

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
improper probe depth - Rrozema - 02-23-2012, 01:00 PM
RE: improper probe depth - rapidrhrep - 02-23-2012, 01:51 PM
RE: improper probe depth - Rrozema - 02-23-2012, 02:22 PM
RE: improper probe depth - Rrozema - 02-28-2012, 08:44 AM
RE: improper probe depth - rapidrhrep - 03-01-2012, 07:43 AM
RE: improper probe depth - CC Solutions - 03-01-2012, 12:47 PM
RE: improper probe depth - Rubensgt40 - 03-04-2012, 03:56 PM
RE: improper probe depth - CCR - 03-09-2012, 06:14 AM
RE: improper probe depth - GP-CA - 03-23-2012, 02:24 PM
RE: improper probe depth - Ernesto - 03-23-2012, 07:51 PM
RE: improper probe depth - CC Solutions - 03-24-2012, 06:12 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
15 Replies 57,682 Views
Last Post by CC Solutions
01-15-2012, 06:33 PM
10 Replies 38,310 Views
Last Post by CC Solutions
03-24-2011, 07:00 AM
2 Replies 13,962 Views
Last Post by CC Solutions
01-15-2010, 09:43 PM
1 Replies 11,765 Views
Last Post by rthompson
02-20-2009, 12:54 PM

Users browsing this thread:
1 Guest(s)