Whats a non-approved special adhesive mean? I've never heard that before, jeez

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

11-16-2011, 06:52 PM #62
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Unapproved. He sold the customer on magic glue that isn't magic at all.

11-16-2011, 07:12 PM #63
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
(11-16-2011, 06:52 PM)eaadams Wrote:  Unapproved. He sold the customer on magic glue that isn't magic at all.

Uapproved for what flooring and by whom? Can't you be more specific, I ain't no mind reader here.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

11-16-2011, 07:26 PM #64
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
We as the manufacture only allow three different adhesives. This guy bought his own and he is now on his own.

11-17-2011, 07:56 AM #65
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
(11-16-2011, 07:26 PM)eaadams Wrote:  We as the manufacture only allow three different adhesives. This guy bought his own and he is now on his own.

There's my point right there.

Manufacturers will quickly wash their hands of jobs that don't follow their requirements or use unapproved materials. And they have the right to! They know what they need to have to perform as designed.


JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 6,586 Views
Last Post by eaadams
05-04-2016, 08:39 PM
3 Replies 17,198 Views
Last Post by CC Solutions
08-20-2012, 07:07 PM
49 Replies 155,091 Views
Last Post by Ernesto
12-08-2011, 06:03 PM
 high rh in concrete
chas04344
2 Replies 15,276 Views
Last Post by chas04344
09-11-2009, 07:33 PM

Users browsing this thread:
2 Guest(s)