Quote:Hee hee, whats the odds? Get us a boxing ring. Can I bet on myself?

I DID get you a boxing ring- I started a thread on reliability of MMS with high RH readings! It doesn't take much with you blokes.... Big Grin Jason, I expect royalties from the takings please. Cool

Still, I'm all the better for it because these debates make for teachable moments, to use an Obamaism.

Quote:Now for your claim that any after the fact high reading will void any warranty. Thats complete nonsense. If that were true there would be no flooring going down and no glue sales.

As much as I'm inclined to agree with this, I think generally most contractors approach a job with eyes wide open- namely, that if a manufacturer wants to sneak out of a warranty, if it gets deep into litigation, they will find a way somehow.



The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher









Messages In This Thread
MMS- Are some unreliable with high RH? - Rubensgt40 - 11-06-2011, 02:24 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-06-2011, 03:25 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-06-2011, 06:19 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-06-2011, 08:01 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 07:23 AM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-07-2011, 02:51 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 02:56 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-07-2011, 03:22 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 04:16 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-07-2011, 07:24 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-08-2011, 07:27 AM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-08-2011, 09:43 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-08-2011, 09:59 AM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-08-2011, 02:27 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-08-2011, 02:50 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-08-2011, 03:34 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-09-2011, 07:20 AM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-09-2011, 07:47 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-09-2011, 09:34 AM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-09-2011, 05:51 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-09-2011, 06:20 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-09-2011, 06:57 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-09-2011, 07:28 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 07:45 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 09:32 AM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-10-2011, 03:40 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 05:13 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-10-2011, 05:16 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 07:08 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-10-2011, 07:30 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 07:34 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 08:06 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 08:09 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 08:20 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 08:33 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 09:03 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-11-2011, 07:12 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 07:28 AM
RE: MMS- Are some unreliable with high RH? - EWagner - 11-11-2011, 10:08 AM
RE: MMS- Are some unreliable with high RH? - rapidrhrep - 11-11-2011, 10:18 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 10:22 AM
RE: MMS- Are some unreliable with high RH? - rapidrhrep - 11-11-2011, 10:31 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 10:34 AM
RE: MMS- Are some unreliable with high RH? - rapidrhrep - 11-11-2011, 10:52 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 10:59 AM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-11-2011, 04:13 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-11-2011, 04:16 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-11-2011, 04:21 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-11-2011, 05:56 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-13-2011, 06:00 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-13-2011, 06:07 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-13-2011, 08:01 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-13-2011, 08:21 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-16-2011, 11:49 AM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 12:20 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-16-2011, 12:31 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 04:45 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-16-2011, 04:57 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 05:18 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 06:23 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 06:35 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 06:52 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 07:12 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 07:26 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-17-2011, 07:56 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 2,677 Views
Last Post by eaadams
05-04-2016, 08:39 PM
3 Replies 14,237 Views
Last Post by CC Solutions
08-20-2012, 07:07 PM
49 Replies 127,618 Views
Last Post by Ernesto
12-08-2011, 06:03 PM
 high rh in concrete
chas04344
2 Replies 12,936 Views
Last Post by chas04344
09-11-2009, 07:33 PM

Users browsing this thread:
1 Guest(s)