Sorry Stephen, you are wrong. Wink

Read the requirements for the glues you are using and tell me which ones do NOT require a functioning vapor retarder under them.

Sure they'll warrant them as long as there's no problem. If you have a problem, they'll point to the no retarder issue and show you where they require it in their data sheet.

There are methods to guarantee slabs with no vapor retarder under them, but gluing and praying isn't the way! Dodgy

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
MMS- Are some unreliable with high RH? - Rubensgt40 - 11-06-2011, 02:24 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-06-2011, 03:25 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-06-2011, 06:19 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-06-2011, 08:01 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 07:23 AM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-07-2011, 02:51 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 02:56 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-07-2011, 03:22 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 04:16 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-07-2011, 07:24 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-08-2011, 07:27 AM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-08-2011, 09:43 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-08-2011, 09:59 AM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-08-2011, 02:27 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-08-2011, 02:50 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-08-2011, 03:34 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-09-2011, 07:20 AM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-09-2011, 07:47 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-09-2011, 09:34 AM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-09-2011, 05:51 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-09-2011, 06:20 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-09-2011, 06:57 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-09-2011, 07:28 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 07:45 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 09:32 AM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-10-2011, 03:40 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 05:13 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-10-2011, 05:16 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 07:08 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-10-2011, 07:30 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 07:34 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 08:06 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 08:09 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 08:20 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 08:33 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 09:03 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-11-2011, 07:12 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 07:28 AM
RE: MMS- Are some unreliable with high RH? - EWagner - 11-11-2011, 10:08 AM
RE: MMS- Are some unreliable with high RH? - rapidrhrep - 11-11-2011, 10:18 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 10:22 AM
RE: MMS- Are some unreliable with high RH? - rapidrhrep - 11-11-2011, 10:31 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 10:34 AM
RE: MMS- Are some unreliable with high RH? - rapidrhrep - 11-11-2011, 10:52 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 10:59 AM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-11-2011, 04:13 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-11-2011, 04:16 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-11-2011, 04:21 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-11-2011, 05:56 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-13-2011, 06:00 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-13-2011, 06:07 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-13-2011, 08:01 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-13-2011, 08:21 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-16-2011, 11:49 AM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 12:20 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-16-2011, 12:31 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 04:45 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-16-2011, 04:57 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 05:18 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 06:23 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 06:35 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 06:52 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 07:12 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 07:26 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-17-2011, 07:56 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 5,507 Views
Last Post by eaadams
05-04-2016, 08:39 PM
3 Replies 16,454 Views
Last Post by CC Solutions
08-20-2012, 07:07 PM
49 Replies 147,883 Views
Last Post by Ernesto
12-08-2011, 06:03 PM
 high rh in concrete
chas04344
2 Replies 14,720 Views
Last Post by chas04344
09-11-2009, 07:33 PM

Users browsing this thread:
1 Guest(s)