(11-10-2011, 07:08 PM)CC Solutions Wrote:  If your readings are under the manufacturer's upper limit and you meet all the rest of the requirements, you will have a warranty.

Nope, I've never seen a flooring manufacturer warrant a floor based on initial testing. If you have a failure and at failure time there is higher moisture than specs allow, the manufacturer walks. Needless to say, if you look at anything hard enough you can always find something to void a warranty.

(11-10-2011, 07:08 PM)CC Solutions Wrote:  There are hundreds of products that claim to 'go to 95%' or more. Why not stick with the three or four that actually work? Huh

Yep I agree. I was looking at the products specs, only ok for tile, not resilient. So it is ... kinda a joke. I'll stick with the four products I know to work but the issue is always that I have to make sure subs don't use products like that.








Messages In This Thread
MMS- Are some unreliable with high RH? - Rubensgt40 - 11-06-2011, 02:24 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-06-2011, 03:25 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-06-2011, 06:19 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-06-2011, 08:01 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 07:23 AM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-07-2011, 02:51 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 02:56 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-07-2011, 03:22 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 04:16 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-07-2011, 07:24 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-08-2011, 07:27 AM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-08-2011, 09:43 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-08-2011, 09:59 AM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-08-2011, 02:27 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-08-2011, 02:50 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-08-2011, 03:34 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-09-2011, 07:20 AM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-09-2011, 07:47 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-09-2011, 09:34 AM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-09-2011, 05:51 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-09-2011, 06:20 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-09-2011, 06:57 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-09-2011, 07:28 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 07:45 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 09:32 AM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-10-2011, 03:40 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 05:13 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-10-2011, 05:16 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 07:08 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-10-2011, 07:30 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 07:34 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 08:06 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 08:09 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 08:20 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-10-2011, 08:33 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-10-2011, 09:03 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-11-2011, 07:12 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 07:28 AM
RE: MMS- Are some unreliable with high RH? - EWagner - 11-11-2011, 10:08 AM
RE: MMS- Are some unreliable with high RH? - rapidrhrep - 11-11-2011, 10:18 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 10:22 AM
RE: MMS- Are some unreliable with high RH? - rapidrhrep - 11-11-2011, 10:31 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 10:34 AM
RE: MMS- Are some unreliable with high RH? - rapidrhrep - 11-11-2011, 10:52 AM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-11-2011, 10:59 AM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-11-2011, 04:13 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-11-2011, 04:16 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-11-2011, 04:21 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-11-2011, 05:56 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-13-2011, 06:00 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-13-2011, 06:07 PM
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-13-2011, 08:01 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-13-2011, 08:21 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-16-2011, 11:49 AM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 12:20 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-16-2011, 12:31 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 04:45 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-16-2011, 04:57 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 05:18 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 06:23 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 06:35 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 06:52 PM
RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011, 07:12 PM
RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011, 07:26 PM
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-17-2011, 07:56 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 3,629 Views
Last Post by eaadams
05-04-2016, 08:39 PM
3 Replies 14,972 Views
Last Post by CC Solutions
08-20-2012, 07:07 PM
49 Replies 133,693 Views
Last Post by Ernesto
12-08-2011, 06:03 PM
 high rh in concrete
chas04344
2 Replies 13,500 Views
Last Post by chas04344
09-11-2009, 07:33 PM

Users browsing this thread:
2 Guest(s)