I agree with you Ray the hood method ASTM F2420 is a similar measurement to the calcium chloride method yet the hood method is measuring the amount of free water in the slab while the calcium chloride test is measuring moisture vapor both of these test reflect a 1/4" to 1/2" of the slabs thickness, ASTM F2170 measures at 40% of the slab depth. Our testing lab has performed all three of these test and have not found a true correlation between the hood method ASTM F2420 and the in situ probe method ASTM F2170 we have found though at ideal conditions the hood method has been five to eight percent lower than the in situ probe. In closing when doing an investigation in flooring failure we chose ASTM F2170 due to the depth the test measures and to the lower chance of tester’s error during placement.

Respectfully
Trever Shiplee








Messages In This Thread
Concrete Hood Method - Blake McFee - 03-25-2009, 09:18 AM
RE: Concrete Hood Method - rthompson - 04-24-2009, 09:49 AM
RE: Concrete Hood Method - Trever Shiplee - 04-29-2009, 11:27 PM
RE: Concrete Hood Method - RCConcrete Consulting - 09-21-2009, 05:31 PM
RE: Concrete Hood Method - WeldKaye - 10-21-2009, 09:41 PM
RE: Concrete Hood Method - Blake McFee - 10-23-2009, 10:02 AM
RE: Concrete Hood Method - CC Solutions - 12-16-2009, 11:39 AM
RE: Concrete Hood Method - RCConcrete Consulting - 12-16-2009, 03:31 PM
RE: Concrete Hood Method - CC Solutions - 12-17-2009, 09:33 AM
RE: Concrete Hood Method - eaadams - 11-08-2013, 01:41 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 11,155 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 28,031 Views
Last Post by eaadams
05-19-2014, 10:55 AM
35 Replies 100,512 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 14,396 Views
Last Post by eaadams
01-30-2013, 04:43 PM
32 Replies 91,797 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
0 Replies 5,794 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 73,574 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
37 Replies 105,511 Views
Last Post by CC Solutions
09-20-2011, 10:07 AM
12 Replies 41,385 Views
Last Post by CC Solutions
06-21-2011, 11:47 AM
8 Replies 25,416 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
1 Guest(s)