false high test results
  • 0 Vote(s) - 0 Average


10-26-2011, 11:10 AM #2
rapidrhrep Concrete Moisture Tutor **
Status: Offline Posts:85 Threads:3 Joined:Aug 2011
EA:

Our webinar actually touches on this. The testing company you spoke with is inaccurate. The dust will not cause a false high overall. The dust MAY slow the equilibration of the probe in the hole. These two explanations are very different. Bottomline, it is important to get that hole clean so you can take full advantage of all of the positive things the Rapid RH brings to the table.

Thanks,

Jason








Messages In This Thread
false high test results - eaadams - 10-25-2011, 08:57 PM
RE: false high test results - rapidrhrep - 10-26-2011, 11:10 AM
RE: false high test results - eaadams - 10-26-2011, 12:11 PM
RE: false high test results - Ernesto - 10-26-2011, 04:47 PM
RE: false high test results - eaadams - 10-26-2011, 05:21 PM
RE: false high test results - rapidrhrep - 10-26-2011, 07:05 PM
RE: false high test results - eaadams - 10-26-2011, 07:11 PM
RE: false high test results - Ernesto - 10-26-2011, 07:17 PM
RE: false high test results - eaadams - 10-26-2011, 09:43 PM
RE: false high test results - CC Solutions - 10-28-2011, 11:47 AM
RE: false high test results - Ernesto - 10-28-2011, 02:03 PM
RE: false high test results - CC Solutions - 10-28-2011, 02:12 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
9 Replies 17,473 Views
Last Post by Ernesto
04-16-2014, 03:49 PM
1 Replies 7,262 Views
Last Post by CC Solutions
09-01-2013, 07:56 AM
7 Replies 25,294 Views
Last Post by Rubensgt40
05-09-2012, 04:35 PM

Users browsing this thread:
1 Guest(s)