10-06-2011, 09:20 PM #6
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
If you get t-shirts printed, send me one Tongue

We're in the process of tightening up the standards now. BTW we reference ASTM F2170 in ours (or we will, fairly soon). As I see happens in the US, the more the standards are refined, the more manufacturers get on board and write up their specs accordingly.

At the moment, we are still emerging from moisture content as the testing requirement and formally moving to RH. The hood method is catching on.

After studying this forum (and Wagner's products) that will have to change.

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher









Messages In This Thread
Ambient humidity vs. RH - Rubensgt40 - 10-04-2011, 09:29 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-06-2011, 06:41 AM
RE: Ambient humidity vs. RH - Ernesto - 10-06-2011, 03:43 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-06-2011, 05:16 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-06-2011, 06:43 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-06-2011, 09:20 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-07-2011, 06:07 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-08-2011, 12:24 AM
RE: Ambient humidity vs. RH - Ernesto - 10-08-2011, 01:42 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-09-2011, 12:58 AM
RE: Ambient humidity vs. RH - eblakewi - 10-10-2011, 11:21 AM
RE: Ambient humidity vs. RH - CC Solutions - 10-10-2011, 11:37 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-10-2011, 02:53 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-10-2011, 03:47 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-11-2011, 04:32 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-12-2011, 06:15 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-13-2011, 09:12 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-14-2011, 06:12 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-16-2011, 02:42 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-16-2011, 06:09 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 3,058 Views
Last Post by CC Solutions
05-17-2016, 08:22 PM
5 Replies 18,508 Views
Last Post by CC Solutions
08-28-2011, 02:02 PM
10 Replies 33,530 Views
Last Post by CC Solutions
03-24-2011, 07:00 AM
11 Replies 37,742 Views
Last Post by CC Solutions
05-11-2010, 03:22 PM
7 Replies 26,579 Views
Last Post by CC Solutions
12-17-2009, 12:16 PM
1 Replies 10,718 Views
Last Post by rthompson
02-20-2009, 01:08 PM

Users browsing this thread:
1 Guest(s)