Well, I guess the all knowing rapidrh experts are not going to chime in on this one or my question about static electricity. sigh

This does not discribe me Ernesto but I will take a swing at your question, and yes you do come up with some good ones. Static electricity is an issue, as with any electrical product. Usually, once assembled, especially in the plastic, you have a buffer. With that being said, we have not specifically tested the vacuuming of a Rapid RH 4.0 sensor and issues with static electricity. I can tell you that many people do do it.

@JD the biggest reason I would not do what you are stating is that the standard specifically says not to.

Have a good weekend gents!

Jason








Messages In This Thread
Using compressed air to clean out the concrete hole. - CC Solutions - 10-04-2011, 04:08 PM
RE: Using compressed air to clean out the concrete hole. - Ernesto - 10-06-2011, 03:48 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-06-2011, 06:30 PM
RE: Using compressed air to clean out the concrete hole. - Ernesto - 10-06-2011, 07:17 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-07-2011, 06:05 AM
RE: Using compressed air to clean out the concrete hole. - Ernesto - 10-07-2011, 07:06 AM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-07-2011, 07:26 AM
RE: Using compressed air to clean out the concrete hole. - rapidrhrep - 10-07-2011, 04:01 PM
RE: Using compressed air to clean out the concrete hole. - Ernesto - 10-07-2011, 06:35 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-09-2011, 10:35 AM
RE: Using compressed air to clean out the concrete hole. - rapidrhrep - 10-10-2011, 08:40 AM
RE: Using compressed air to clean out the concrete hole. - eaadams - 10-12-2011, 04:05 PM
RE: Using compressed air to clean out the concrete hole. - Ernesto - 10-12-2011, 06:41 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-12-2011, 06:47 PM
RE: Using compressed air to clean out the concrete hole. - eaadams - 10-12-2011, 06:52 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-12-2011, 07:13 PM
RE: Using compressed air to clean out the concrete hole. - FloorMedic's - 10-12-2011, 09:25 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-13-2011, 06:22 AM
RE: Using compressed air to clean out the concrete hole. - eaadams - 10-13-2011, 02:54 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-13-2011, 03:02 PM
RE: Using compressed air to clean out the concrete hole. - Ernesto - 10-13-2011, 03:25 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-13-2011, 03:28 PM
RE: Using compressed air to clean out the concrete hole. - Ernesto - 10-13-2011, 03:52 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-14-2011, 06:24 AM
RE: Using compressed air to clean out the concrete hole. - Ernesto - 10-14-2011, 12:52 PM
RE: Using compressed air to clean out the concrete hole. - CC Solutions - 10-14-2011, 01:06 PM
RE: Using compressed air to clean out the concrete hole. - rthompson - 11-30-2011, 11:29 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
5 Replies 32,842 Views
Last Post by CC Solutions
12-04-2013, 08:46 AM

Users browsing this thread:
1 Guest(s)