Can tape over the probe cause erroneous readings?
  • 0 Vote(s) - 0 Average


08-01-2013, 04:08 AM #21
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
LawyersDodgy. Since ASTM 2170 endorses sealing, I'm not so sure a lawyer would go down that path. A pure silicone I suspect would be preferable, or even a urethane. I've been using the Loctite for well over a year now and noticed no effect on my readings + or -. Plus, you just about have to use a utility knife or screwdriver to break the bond loose once it dries.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

06-02-2014, 10:17 PM #22
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Here is a video link with Jason saying Tape is AOK!
http://www.wagnermeters.com/rapid-rh-newsletters/may-2014-rapid-rh-newsletter/?utm_medium=email&utm_source=infusionsoft&utm_campaign=WMCF+Newsletter&utm_content=Video&inf_contact_key=4a3188b4db758aafc2fc1c5685d13e82ebe810496325e402b8fdc47394fb5e2b

06-03-2014, 03:49 PM #23
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
The sensor is reading the rh from underneath it, not from up top. The underneath part is sealed from the top is it not? If so then what ever you cap it with would not matter temp and ambient rh wise as long as debris and water does not enter it.

How about an old wax seal like the brits used to use?

(06-02-2014, 10:17 PM)eaadams Wrote:  Here is a video link with Jason saying Tape is AOK!
http://www.wagnermeters.com/rapid-rh-newsletters/may-2014-rapid-rh-newsletter/?utm_medium=email&utm_source=infusionsoft&utm_campaign=WMCF+Newsletter&utm_content=Video&inf_contact_key=4a3188b4db758aafc2fc1c5685d13e82ebe810496325e402b8fdc47394fb5e2b

Upside down? Big Grin

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com