I believe caulk does have some water in it. As minimal as it is who would want to get grilled on it in court.

How about pure silicone? Probably sticks and seals better than caulk.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
Can tape over the probe cause erroneous readings? - CC Solutions - 10-04-2011, 04:00 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 10-12-2011, 04:07 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 10-12-2011, 06:50 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 10-12-2011, 06:54 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 06-25-2012, 11:38 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 06-26-2012, 05:52 AM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-01-2012, 04:57 AM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-01-2012, 08:42 AM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-01-2012, 09:09 AM
RE: Can tape over the probe cause erroneous readings? - rthompson - 07-03-2012, 12:44 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-03-2012, 01:20 PM
RE: Can tape over the probe cause erroneous readings? - rthompson - 07-03-2012, 02:02 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-03-2012, 02:17 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 07-09-2012, 01:27 PM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-10-2012, 10:47 AM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-12-2012, 06:06 AM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-12-2012, 07:41 AM
RE: Can tape over the probe cause erroneous readings? - eaadams - 07-12-2012, 12:50 PM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-24-2013, 04:47 PM
RE: Can tape over the probe cause erroneous readings? - Ernesto - 07-31-2013, 01:05 PM
RE: Can tape over the probe cause erroneous readings? - CCR - 08-01-2013, 04:08 AM
RE: Can tape over the probe cause erroneous readings? - eaadams - 06-02-2014, 10:17 PM
RE: Can tape over the probe cause erroneous readings? - Ernesto - 06-03-2014, 03:49 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 14,047 Views
Last Post by CC Solutions
09-02-2011, 06:25 AM

Users browsing this thread:
1 Guest(s)