Very interesting.

I need to find out how Wagner has redesigned the test probes now that the requirement for a full sleeve is in effect. The previous probes would breathe, they have holes in them, but are they designed to breathe a certain percentage to mimic porous concrete?

If they allow moisture to escape from the test hole, how will 3 month old tests correlate with new tests? Huh

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Can tape over the probe cause erroneous readings? - CC Solutions - 10-04-2011, 04:00 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 10-12-2011, 04:07 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 10-12-2011, 06:50 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 10-12-2011, 06:54 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 06-25-2012, 11:38 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 06-26-2012, 05:52 AM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-01-2012, 04:57 AM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-01-2012, 08:42 AM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-01-2012, 09:09 AM
RE: Can tape over the probe cause erroneous readings? - rthompson - 07-03-2012, 12:44 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-03-2012, 01:20 PM
RE: Can tape over the probe cause erroneous readings? - rthompson - 07-03-2012, 02:02 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-03-2012, 02:17 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 07-09-2012, 01:27 PM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-10-2012, 10:47 AM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-12-2012, 06:06 AM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-12-2012, 07:41 AM
RE: Can tape over the probe cause erroneous readings? - eaadams - 07-12-2012, 12:50 PM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-24-2013, 04:47 PM
RE: Can tape over the probe cause erroneous readings? - Ernesto - 07-31-2013, 01:05 PM
RE: Can tape over the probe cause erroneous readings? - CCR - 08-01-2013, 04:08 AM
RE: Can tape over the probe cause erroneous readings? - eaadams - 06-02-2014, 10:17 PM
RE: Can tape over the probe cause erroneous readings? - Ernesto - 06-03-2014, 03:49 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 13,456 Views
Last Post by CC Solutions
09-02-2011, 06:25 AM

Users browsing this thread:
1 Guest(s)