Debris in the Sensor
  • 0 Vote(s) - 0 Average


07-23-2013, 08:48 PM #20
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Which leads me to ask again,

Are the vent holes in the bottom of the Wagner probes calibrated to accurately mimic the drying of the surrounding concrete over months of testing?? Tongue

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Debris in the Sensor - Ernesto - 10-03-2011, 01:18 PM
RE: Debris in the Sensor - CC Solutions - 10-03-2011, 04:06 PM
RE: Debris in the Sensor - Ernesto - 10-04-2011, 02:13 PM
RE: Debris in the Sensor - CC Solutions - 10-04-2011, 02:52 PM
RE: Debris in the Sensor - Ernesto - 10-04-2011, 03:23 PM
RE: Debris in the Sensor - CC Solutions - 10-04-2011, 03:56 PM
RE: Debris in the Sensor - Ernesto - 10-04-2011, 06:04 PM
RE: Debris in the Sensor - CC Solutions - 10-06-2011, 11:31 AM
RE: Debris in the Sensor - Ernesto - 10-06-2011, 03:40 PM
RE: Debris in the Sensor - CCR - 07-19-2013, 04:21 PM
RE: Debris in the Sensor - CC Solutions - 07-19-2013, 04:41 PM
RE: Debris in the Sensor - CCR - 07-19-2013, 05:10 PM
RE: Debris in the Sensor - CCR - 07-20-2013, 04:54 AM
RE: Debris in the Sensor - CC Solutions - 07-22-2013, 09:09 AM
RE: Debris in the Sensor - CCR - 07-22-2013, 12:10 PM
RE: Debris in the Sensor - rapidrhrep - 07-23-2013, 11:11 AM
RE: Debris in the Sensor - CCR - 07-23-2013, 11:30 AM
RE: Debris in the Sensor - CC Solutions - 07-23-2013, 08:36 PM
RE: Debris in the Sensor - rapidrhrep - 07-23-2013, 08:46 PM
RE: Debris in the Sensor - CC Solutions - 07-23-2013, 08:48 PM
RE: Debris in the Sensor - rapidrhrep - 07-23-2013, 08:55 PM
RE: Debris in the Sensor - CCR - 07-24-2013, 08:15 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
1 Replies 11,670 Views
Last Post by rthompson
10-01-2008, 03:46 PM

Users browsing this thread:
1 Guest(s)