Is RapidRH 4.0 compatible with ASTM 2170-11?

NO manufacturer in the marketplace, that I am aware of, is 100% compatible with this latest revision. The Rapid RH is one of the closest, as you can see based on my quick outline, and would see even clearer if you had the revision and saw the drawings. There will be a transitional phase for all, some worse than others, in order to attempt to make RH readings more reproducible among the different devices currently available in the marketplace.

Jason said the sleeve must be the entire depth of the hole. He did not say if the sleeve can be two piece.

JD-I really liked this comment.Undecided

Jason








Messages In This Thread
ASTM 2170-11 - eaadams - 09-30-2011, 04:00 PM
RE: ASTM 2170-11 - CC Solutions - 10-01-2011, 05:35 AM
RE: ASTM 2170-11 - eaadams - 10-01-2011, 08:36 AM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 07:05 AM
RE: ASTM 2170-11 - rapidrhrep - 10-03-2011, 08:23 AM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 08:36 AM
RE: ASTM 2170-11 - Ernesto - 10-03-2011, 01:10 PM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 01:16 PM
RE: ASTM 2170-11 - eaadams - 10-03-2011, 01:27 PM
RE: ASTM 2170-11 - Ernesto - 10-03-2011, 02:15 PM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 02:21 PM
RE: ASTM 2170-11 - Ernesto - 10-03-2011, 02:23 PM
RE: ASTM 2170-11 - rapidrhrep - 10-03-2011, 03:30 PM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 04:10 PM
RE: ASTM 2170-11 - eaadams - 10-12-2011, 04:31 PM
RE: ASTM 2170-11 - rapidrhrep - 10-12-2011, 04:54 PM
RE: ASTM 2170-11 - CC Solutions - 10-12-2011, 07:00 PM
RE: ASTM 2170-11 - Ernesto - 10-13-2011, 06:50 AM
RE: ASTM 2170-11 - CC Solutions - 10-13-2011, 07:06 AM
RE: ASTM 2170-11 - Ernesto - 10-13-2011, 02:59 PM
RE: ASTM 2170-11 - Rubensgt40 - 10-16-2011, 03:47 PM
RE: ASTM 2170-11 - CC Solutions - 10-16-2011, 05:53 PM
RE: ASTM 2170-11 - Rubensgt40 - 10-16-2011, 11:13 PM
RE: ASTM 2170-11 - CC Solutions - 10-17-2011, 06:00 AM
RE: ASTM 2170-11 - rapidrhrep - 10-17-2011, 08:38 AM
RE: ASTM 2170-11 - CC Solutions - 10-17-2011, 08:49 AM
RE: ASTM 2170-11 - eaadams - 10-25-2011, 09:04 PM
RE: ASTM 2170-11 - Rubensgt40 - 10-31-2011, 05:30 AM
RE: ASTM 2170-11 - eaadams - 10-31-2011, 11:17 AM
RE: ASTM 2170-11 - CC Solutions - 10-31-2011, 11:31 AM
RE: ASTM 2170-11 - rapidrhrep - 10-31-2011, 12:41 PM
RE: ASTM 2170-11 - CC Solutions - 10-31-2011, 01:57 PM
RE: ASTM 2170-11 - eaadams - 10-31-2011, 11:36 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
0 Replies 4,758 Views
Last Post by eaadams
04-15-2014, 09:33 AM
1 Replies 8,952 Views
Last Post by CC Solutions
02-25-2014, 05:54 PM

Users browsing this thread:
1 Guest(s)