ASTM 2170-11
  • 0 Vote(s) - 0 Average


10-03-2011, 01:10 PM #7
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
(10-03-2011, 08:36 AM)CC Solutions Wrote:  Thanks for the update Jason!

Yeah power steering... Who would have seen that coming?

Okay, are you changing the probes again to have full height sleeves? Or will a tube in a tube work to meet the requirement?

Ea, I believe the wagner sensors don't need a sleeve to the top because they only read that teensy weensy airspace at the bottom of the hole. Is that what your talking about?


Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
ASTM 2170-11 - eaadams - 09-30-2011, 04:00 PM
RE: ASTM 2170-11 - CC Solutions - 10-01-2011, 05:35 AM
RE: ASTM 2170-11 - eaadams - 10-01-2011, 08:36 AM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 07:05 AM
RE: ASTM 2170-11 - rapidrhrep - 10-03-2011, 08:23 AM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 08:36 AM
RE: ASTM 2170-11 - Ernesto - 10-03-2011, 01:10 PM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 01:16 PM
RE: ASTM 2170-11 - eaadams - 10-03-2011, 01:27 PM
RE: ASTM 2170-11 - Ernesto - 10-03-2011, 02:15 PM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 02:21 PM
RE: ASTM 2170-11 - Ernesto - 10-03-2011, 02:23 PM
RE: ASTM 2170-11 - rapidrhrep - 10-03-2011, 03:30 PM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 04:10 PM
RE: ASTM 2170-11 - eaadams - 10-12-2011, 04:31 PM
RE: ASTM 2170-11 - rapidrhrep - 10-12-2011, 04:54 PM
RE: ASTM 2170-11 - CC Solutions - 10-12-2011, 07:00 PM
RE: ASTM 2170-11 - Ernesto - 10-13-2011, 06:50 AM
RE: ASTM 2170-11 - CC Solutions - 10-13-2011, 07:06 AM
RE: ASTM 2170-11 - Ernesto - 10-13-2011, 02:59 PM
RE: ASTM 2170-11 - Rubensgt40 - 10-16-2011, 03:47 PM
RE: ASTM 2170-11 - CC Solutions - 10-16-2011, 05:53 PM
RE: ASTM 2170-11 - Rubensgt40 - 10-16-2011, 11:13 PM
RE: ASTM 2170-11 - CC Solutions - 10-17-2011, 06:00 AM
RE: ASTM 2170-11 - rapidrhrep - 10-17-2011, 08:38 AM
RE: ASTM 2170-11 - CC Solutions - 10-17-2011, 08:49 AM
RE: ASTM 2170-11 - eaadams - 10-25-2011, 09:04 PM
RE: ASTM 2170-11 - Rubensgt40 - 10-31-2011, 05:30 AM
RE: ASTM 2170-11 - eaadams - 10-31-2011, 11:17 AM
RE: ASTM 2170-11 - CC Solutions - 10-31-2011, 11:31 AM
RE: ASTM 2170-11 - rapidrhrep - 10-31-2011, 12:41 PM
RE: ASTM 2170-11 - CC Solutions - 10-31-2011, 01:57 PM
RE: ASTM 2170-11 - eaadams - 10-31-2011, 11:36 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
0 Replies 3,853 Views
Last Post by eaadams
04-15-2014, 09:33 AM
1 Replies 7,430 Views
Last Post by CC Solutions
02-25-2014, 05:54 PM

Users browsing this thread:
1 Guest(s)