#Login Register
Self consolidating concrete (SCC)
  • 0 Vote(s) - 0 Average


05-07-2012, 01:34 PM #31
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
I am not familiar with self consolidating concrete, but a super plasticizer typically helps reduce cracking because it reduces the amount of excess water needed to place the concrete.

Are these surface cracks or are they deeper? When you say stress cracks I think of shrinkage cracks, the concrete is restrained by steel, sub-soil and other factors and as it dries and shrinks there is a great amount of stress built up and it has to shrink, so it cracks.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

05-08-2012, 04:24 AM #32
JDJR Newbie *
Status: Offline Posts:5 Threads:2 Joined:Sep 2009
they are mostly surface cracks - some bigger then others.
they told me that the Super P dries the concrete so fast that these cracks are very common.

05-08-2012, 07:04 AM #33
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
A super plasticizer allows you to reduce the amount of mix water which could limit the amount of bleed water causing the surface to dry more rapidly.

To insure proper surface curing you can always wet cure or use a curing spray. This will maximize surface water and promote cement hydration at the surface.

Surface cracks are commonly cosmetic and don't go very deep.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 12,342 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 31,248 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 41,623 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 106,066 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 15,368 Views
Last Post by eaadams
01-30-2013, 04:43 PM
0 Replies 6,153 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 77,355 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
37 Replies 111,896 Views
Last Post by CC Solutions
09-20-2011, 10:07 AM
12 Replies 43,388 Views
Last Post by CC Solutions
06-21-2011, 11:47 AM
8 Replies 26,791 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
2 Guest(s)