I am not familiar with self consolidating concrete, but a super plasticizer typically helps reduce cracking because it reduces the amount of excess water needed to place the concrete.

Are these surface cracks or are they deeper? When you say stress cracks I think of shrinkage cracks, the concrete is restrained by steel, sub-soil and other factors and as it dries and shrinks there is a great amount of stress built up and it has to shrink, so it cracks.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Self consolidating concrete (SCC) - eaadams - 09-17-2011, 02:07 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-17-2011, 03:46 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-18-2011, 09:23 AM
RE: Self consolidating concrete (SCC) - rthompson - 09-28-2011, 05:37 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-28-2011, 08:14 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-29-2011, 08:29 AM
RE: Self consolidating concrete (SCC) - eaadams - 09-29-2011, 05:48 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-29-2011, 07:42 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-29-2011, 08:23 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-30-2011, 08:15 AM
RE: Self consolidating concrete (SCC) - Ernesto - 09-30-2011, 12:30 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-30-2011, 04:02 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-30-2011, 05:36 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-30-2011, 06:09 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-01-2011, 05:29 AM
RE: Self consolidating concrete (SCC) - Ernesto - 10-01-2011, 07:39 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-01-2011, 08:06 AM
RE: Self consolidating concrete (SCC) - eaadams - 10-01-2011, 08:39 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-02-2011, 12:07 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-02-2011, 05:07 PM
RE: Self consolidating concrete (SCC) - eaadams - 10-02-2011, 07:02 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-03-2011, 05:58 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-03-2011, 07:31 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-03-2011, 08:32 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-07-2011, 06:09 AM
RE: Self consolidating concrete (SCC) - EWagner - 10-13-2011, 10:18 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-13-2011, 10:38 AM
RE: Self consolidating concrete (SCC) - foxgeorge - 12-15-2011, 12:59 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 12-15-2011, 11:41 AM
RE: Self consolidating concrete (SCC) - JDJR - 05-07-2012, 12:55 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 05-07-2012, 01:34 PM
RE: Self consolidating concrete (SCC) - JDJR - 05-08-2012, 04:24 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 05-08-2012, 07:04 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 14,308 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 37,083 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 44,843 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 116,401 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 17,217 Views
Last Post by eaadams
01-30-2013, 04:43 PM
0 Replies 6,737 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 83,998 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
37 Replies 122,434 Views
Last Post by CC Solutions
09-20-2011, 10:07 AM
12 Replies 47,124 Views
Last Post by CC Solutions
06-21-2011, 11:47 AM
8 Replies 29,569 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
1 Guest(s)