SSC concrete is a low w/c ratio highly plasticized concrete. It is amazing how it flows and yet the coarse aggregate still remains suspended. The heavy pours do not need to be vibrated like normal concrete. It does dry faster than normal concrete because of the low w/c ratio and less water.
Regards
Rayt








Messages In This Thread
Self consolidating concrete (SCC) - eaadams - 09-17-2011, 02:07 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-17-2011, 03:46 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-18-2011, 09:23 AM
RE: Self consolidating concrete (SCC) - rthompson - 09-28-2011, 05:37 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-28-2011, 08:14 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-29-2011, 08:29 AM
RE: Self consolidating concrete (SCC) - eaadams - 09-29-2011, 05:48 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-29-2011, 07:42 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-29-2011, 08:23 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-30-2011, 08:15 AM
RE: Self consolidating concrete (SCC) - Ernesto - 09-30-2011, 12:30 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-30-2011, 04:02 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-30-2011, 05:36 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-30-2011, 06:09 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-01-2011, 05:29 AM
RE: Self consolidating concrete (SCC) - Ernesto - 10-01-2011, 07:39 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-01-2011, 08:06 AM
RE: Self consolidating concrete (SCC) - eaadams - 10-01-2011, 08:39 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-02-2011, 12:07 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-02-2011, 05:07 PM
RE: Self consolidating concrete (SCC) - eaadams - 10-02-2011, 07:02 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-03-2011, 05:58 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-03-2011, 07:31 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-03-2011, 08:32 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-07-2011, 06:09 AM
RE: Self consolidating concrete (SCC) - EWagner - 10-13-2011, 10:18 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-13-2011, 10:38 AM
RE: Self consolidating concrete (SCC) - foxgeorge - 12-15-2011, 12:59 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 12-15-2011, 11:41 AM
RE: Self consolidating concrete (SCC) - JDJR - 05-07-2012, 12:55 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 05-07-2012, 01:34 PM
RE: Self consolidating concrete (SCC) - JDJR - 05-08-2012, 04:24 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 05-08-2012, 07:04 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 11,232 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 28,213 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 39,882 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 100,869 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 14,458 Views
Last Post by eaadams
01-30-2013, 04:43 PM
0 Replies 5,822 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 73,818 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
37 Replies 105,928 Views
Last Post by CC Solutions
09-20-2011, 10:07 AM
12 Replies 41,527 Views
Last Post by CC Solutions
06-21-2011, 11:47 AM
8 Replies 25,490 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
1 Guest(s)