Question If it is true that SCC has lower permeability than normal concrete, does this mean it dry's slower?
Question Thus resulting in less curling? Or are shrinkage reducing admixtures still greatly needed?

Certainly looks to me that SCC can't be used over a sand blotter layer... which seems like a very good thing for Div 9 people.

Question Is SCC to be tested differently for moisture?

Question Do moisture sealing companies treat SCC differently?

Question Any other things I should know?



Amazing stuff to see on YouTube about SCC.

I think concrete construction is doing an issue on it. That is the current poll on: http://www.concreteconstruction.net/








Messages In This Thread
Self consolidating concrete (SCC) - eaadams - 09-17-2011, 02:07 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-17-2011, 03:46 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-18-2011, 09:23 AM
RE: Self consolidating concrete (SCC) - rthompson - 09-28-2011, 05:37 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-28-2011, 08:14 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-29-2011, 08:29 AM
RE: Self consolidating concrete (SCC) - eaadams - 09-29-2011, 05:48 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-29-2011, 07:42 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-29-2011, 08:23 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-30-2011, 08:15 AM
RE: Self consolidating concrete (SCC) - Ernesto - 09-30-2011, 12:30 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-30-2011, 04:02 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-30-2011, 05:36 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-30-2011, 06:09 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-01-2011, 05:29 AM
RE: Self consolidating concrete (SCC) - Ernesto - 10-01-2011, 07:39 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-01-2011, 08:06 AM
RE: Self consolidating concrete (SCC) - eaadams - 10-01-2011, 08:39 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-02-2011, 12:07 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-02-2011, 05:07 PM
RE: Self consolidating concrete (SCC) - eaadams - 10-02-2011, 07:02 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-03-2011, 05:58 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-03-2011, 07:31 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-03-2011, 08:32 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-07-2011, 06:09 AM
RE: Self consolidating concrete (SCC) - EWagner - 10-13-2011, 10:18 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-13-2011, 10:38 AM
RE: Self consolidating concrete (SCC) - foxgeorge - 12-15-2011, 12:59 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 12-15-2011, 11:41 AM
RE: Self consolidating concrete (SCC) - JDJR - 05-07-2012, 12:55 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 05-07-2012, 01:34 PM
RE: Self consolidating concrete (SCC) - JDJR - 05-08-2012, 04:24 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 05-08-2012, 07:04 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 11,245 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 28,248 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 39,903 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 101,003 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 14,475 Views
Last Post by eaadams
01-30-2013, 04:43 PM
0 Replies 5,827 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 73,880 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
37 Replies 105,990 Views
Last Post by CC Solutions
09-20-2011, 10:07 AM
12 Replies 41,545 Views
Last Post by CC Solutions
06-21-2011, 11:47 AM
8 Replies 25,516 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
1 Guest(s)