I have to get something together for a maintenance supervisor to take to a top 50 (in size) supervisors meeting. So he will take what I give him and present it to them.

I have to explain what moisture is and why their floor is failing. I tested it and it came out at 99% rH. Went outside and in the dessert w/ no watering for the summer, it looks like marsh land, 4' tall green weeds. So I am concluding that it is moisture intrusion to the slab and it is probably spreading under the slab through a sand blotter layer.

Ray, can you point me to some good summation articles you might have done?

I think I will use this as a base: http://www.concreteconstruction.net/concrete-construction/why-are-we-still-having-problems-with-moisture.aspx

I feel like I am playing telephone with concrete moisture and it makes me feel uneasy.








Messages In This Thread
City Supervisors Meeting - eaadams - 08-31-2011, 12:25 PM
RE: City Supervisors Meeting - rthompson - 08-31-2011, 01:20 PM
RE: City Supervisors Meeting - eaadams - 08-31-2011, 01:35 PM
RE: City Supervisors Meeting - CC Solutions - 08-31-2011, 03:02 PM
RE: City Supervisors Meeting - rthompson - 08-31-2011, 11:47 PM
RE: City Supervisors Meeting - eaadams - 09-02-2011, 09:18 AM
RE: City Supervisors Meeting - CC Solutions - 09-02-2011, 09:33 AM
RE: City Supervisors Meeting - Ernesto - 09-03-2011, 02:00 PM
RE: City Supervisors Meeting - CC Solutions - 09-03-2011, 03:54 PM
RE: City Supervisors Meeting - Ernesto - 09-03-2011, 04:41 PM
RE: City Supervisors Meeting - CC Solutions - 09-04-2011, 06:36 AM
RE: City Supervisors Meeting - Ernesto - 09-04-2011, 09:22 AM
RE: City Supervisors Meeting - CC Solutions - 09-04-2011, 10:41 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
5 Replies 11,001 Views
Last Post by rhguru
05-16-2014, 07:53 AM

Users browsing this thread:
1 Guest(s)