I was called to provide a second opinion on a job not 10 miles from my shop (THAT never happens!).

The original installer used Wagner Rapid RH probes but the readings were too high. Then the GC called me and wanted a second opinion. I talked to him for a while, and talked to the first installer (a good client of mine) and the decision was made. The owners want a second opinion, even if it is with the same testing probes. Wink

So I put in three probes today just to validate the readings that the first installer was getting. I'll go back to check them tomorrow, and then on Sunday afternoon (I have a key ---- Small Town USA!).

My objectives on this job:
Gain and foster trust for the Wagner probes. The GC will use them again.
Teach the GC why the slab isn't drying.
Explain the dangers of flooring on a wet slab.
Offer a user friendly and fast mitigation system to eliminate future problems.

Wish me luck! I've never had a job this close to home!!!!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

08-14-2011, 02:11 PM #2
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
The results are in and the probes read exactly the same at 72 hours as they did at 22 hours. They are a bit lower than the first probes that were installed. They are a slight bit deeper in the slab as the installer was told the floor was 4-5 inches thick and I used the 4 inch depth because that's what the blue prints show.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

08-14-2011, 07:56 PM #3
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Different spots, different readings even so slight a depth is what I think. Nothing spectacular should happen if the slab is protected.

Quote:My objectives on this job:
Offer a user friendly and fast mitigation system to eliminate future problems.

Isin't that what it's always about?

I had a guy call me for moisture testing on a commercial job last week, just my luck I was in San Diego on a short vacation.Sad

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
6 Replies 25,155 Views
Last Post by eaadams
03-23-2012, 09:29 AM
15 Replies 56,858 Views
Last Post by CC Solutions
01-15-2012, 06:33 PM
49 Replies 144,947 Views
Last Post by Ernesto
12-08-2011, 06:03 PM
1 Replies 10,029 Views
Last Post by EWagner
06-20-2011, 01:53 PM
11 Replies 38,534 Views
Last Post by CC Solutions
04-23-2011, 08:34 PM
5 Replies 20,180 Views
Last Post by CC Solutions
02-05-2011, 09:36 AM
6 Replies 21,404 Views
Last Post by CC Solutions
11-19-2010, 05:26 PM
1 Replies 11,890 Views
Last Post by rthompson
10-15-2008, 11:00 AM

Users browsing this thread:
1 Guest(s)