I was called to provide a second opinion on a job not 10 miles from my shop (THAT never happens!).

The original installer used Wagner Rapid RH probes but the readings were too high. Then the GC called me and wanted a second opinion. I talked to him for a while, and talked to the first installer (a good client of mine) and the decision was made. The owners want a second opinion, even if it is with the same testing probes. Wink

So I put in three probes today just to validate the readings that the first installer was getting. I'll go back to check them tomorrow, and then on Sunday afternoon (I have a key ---- Small Town USA!).

My objectives on this job:
Gain and foster trust for the Wagner probes. The GC will use them again.
Teach the GC why the slab isn't drying.
Explain the dangers of flooring on a wet slab.
Offer a user friendly and fast mitigation system to eliminate future problems.

Wish me luck! I've never had a job this close to home!!!!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
A GC wants a second opinion, and the first readings were Wagner's! - CC Solutions - 08-11-2011, 05:27 PM
RE: A GC wants a second opinion, and the first readings were Wagner's! - CC Solutions - 08-14-2011, 02:11 PM
RE: A GC wants a second opinion, and the first readings were Wagner's! - Ernesto - 08-14-2011, 07:56 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
6 Replies 25,526 Views
Last Post by eaadams
03-23-2012, 09:29 AM
15 Replies 57,682 Views
Last Post by CC Solutions
01-15-2012, 06:33 PM
49 Replies 147,276 Views
Last Post by Ernesto
12-08-2011, 06:03 PM
1 Replies 10,153 Views
Last Post by EWagner
06-20-2011, 01:53 PM
11 Replies 39,120 Views
Last Post by CC Solutions
04-23-2011, 08:34 PM
5 Replies 20,496 Views
Last Post by CC Solutions
02-05-2011, 09:36 AM
6 Replies 21,708 Views
Last Post by CC Solutions
11-19-2010, 05:26 PM
1 Replies 12,009 Views
Last Post by rthompson
10-15-2008, 11:00 AM

Users browsing this thread:
1 Guest(s)