Another discussion beyond cracks is one of joints....

I read over some of the ardex moisture systems and for some joints they fill with a polyurea before system install, which I found interesting.

I guess a polyurea won't be as hard as an epoxy so it won't some day crack the slu on top and allow a moisture path through the system?

For active expansion joints it looks like they must be honored.








Messages In This Thread
How are you addressing cracks? - CC Solutions - 08-11-2011, 08:03 AM
RE: How are you addressing cracks? - Ernesto - 08-14-2011, 08:16 PM
RE: How are you addressing cracks? - CC Solutions - 08-14-2011, 09:34 PM
RE: How are you addressing cracks? - eaadams - 08-19-2011, 03:56 PM
RE: How are you addressing cracks? - CC Solutions - 08-19-2011, 04:20 PM
RE: How are you addressing cracks? - Ernesto - 08-19-2011, 08:17 PM
RE: How are you addressing cracks? - CC Solutions - 08-19-2011, 08:26 PM
RE: How are you addressing cracks? - Ernesto - 08-19-2011, 08:32 PM
RE: How are you addressing cracks? - CC Solutions - 08-19-2011, 09:00 PM
RE: How are you addressing cracks? - Ernesto - 08-20-2011, 06:40 AM
RE: How are you addressing cracks? - CC Solutions - 08-20-2011, 09:51 PM
RE: How are you addressing cracks? - Ernesto - 08-25-2011, 06:53 PM
RE: How are you addressing cracks? - rthompson - 08-26-2011, 01:55 PM
RE: How are you addressing cracks? - CC Solutions - 08-26-2011, 02:30 PM
RE: How are you addressing cracks? - eaadams - 08-31-2011, 11:53 AM
RE: How are you addressing cracks? - rthompson - 08-31-2011, 01:17 PM
RE: How are you addressing cracks? - CC Solutions - 08-31-2011, 02:54 PM
RE: How are you addressing cracks? - eaadams - 09-14-2011, 01:26 AM
RE: How are you addressing cracks? - CC Solutions - 09-14-2011, 07:07 AM
RE: How are you addressing cracks? - eaadams - 09-14-2011, 06:41 PM
RE: How are you addressing cracks? - Ernesto - 09-14-2011, 07:09 PM
RE: How are you addressing cracks? - CC Solutions - 09-15-2011, 05:40 AM
RE: How are you addressing cracks? - eaadams - 09-15-2011, 12:06 PM
RE: How are you addressing cracks? - CC Solutions - 09-15-2011, 01:10 PM
RE: How are you addressing cracks? - Ernesto - 09-20-2011, 08:14 PM
RE: How are you addressing cracks? - CC Solutions - 09-20-2011, 08:29 PM
RE: How are you addressing cracks? - eaadams - 10-19-2011, 09:55 PM
RE: How are you addressing cracks? - CC Solutions - 10-20-2011, 06:58 AM
RE: How are you addressing cracks? - rthompson - 10-20-2011, 09:38 AM
RE: How are you addressing cracks? - eaadams - 10-20-2011, 05:07 PM
RE: How are you addressing cracks? - Ernesto - 10-20-2011, 07:17 PM
RE: How are you addressing cracks? - CC Solutions - 10-21-2011, 07:02 AM
RE: How are you addressing cracks? - eaadams - 10-21-2011, 09:20 AM