Oh, old slab! Well then moisture can be high in areas where the vapor retarder is compromised and pipes are broken, or any other number of things.

You'll have to ask an adhesive guru about the cutback.... Tongue

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Cold Expansion Joint - eaadams - 08-08-2011, 11:12 AM
RE: Cold Expansion Joint - CC Solutions - 08-08-2011, 11:57 AM
RE: Cold Expansion Joint - eaadams - 08-08-2011, 01:42 PM
RE: Cold Expansion Joint - CC Solutions - 08-08-2011, 02:15 PM
RE: Cold Expansion Joint - eaadams - 08-09-2011, 09:28 PM
RE: Cold Expansion Joint - CC Solutions - 08-09-2011, 09:34 PM
RE: Cold Expansion Joint - eaadams - 08-09-2011, 09:55 PM
RE: Cold Expansion Joint - CC Solutions - 08-09-2011, 10:02 PM
RE: Cold Expansion Joint - Ernesto - 08-14-2011, 08:23 PM
RE: Cold Expansion Joint - eaadams - 08-14-2011, 09:50 PM
RE: Cold Expansion Joint - CC Solutions - 08-15-2011, 04:04 AM
RE: Cold Expansion Joint - Ernesto - 08-16-2011, 08:11 PM
RE: Cold Expansion Joint - CC Solutions - 08-19-2011, 07:14 AM
RE: Cold Expansion Joint - eaadams - 10-21-2011, 06:53 PM
RE: Cold Expansion Joint - CC Solutions - 10-21-2011, 07:30 PM
RE: Cold Expansion Joint - eaadams - 10-21-2011, 07:49 PM
RE: Cold Expansion Joint - CC Solutions - 10-22-2011, 07:24 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post

Users browsing this thread:
2 Guest(s)