Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Owner's rep walks into meeting. She is a tilt up concrete engineer in silicon valley. SWEET. They all came to sences.

Now the rH..... See how dark that slab is. Testing came in from low 80's to 99%. I think the pH is like 12. UGH. So annoying.

For some reason with this one tester every time I get some super high test results. He uses putty to seal the wagner 'cap' to the sleeve / concrete. Might that throw results off?








Messages In This Thread
Cold Expansion Joint - eaadams - 08-08-2011, 11:12 AM
RE: Cold Expansion Joint - CC Solutions - 08-08-2011, 11:57 AM
RE: Cold Expansion Joint - eaadams - 08-08-2011, 01:42 PM
RE: Cold Expansion Joint - CC Solutions - 08-08-2011, 02:15 PM
RE: Cold Expansion Joint - eaadams - 08-09-2011, 09:28 PM
RE: Cold Expansion Joint - CC Solutions - 08-09-2011, 09:34 PM
RE: Cold Expansion Joint - eaadams - 08-09-2011, 09:55 PM
RE: Cold Expansion Joint - CC Solutions - 08-09-2011, 10:02 PM
RE: Cold Expansion Joint - Ernesto - 08-14-2011, 08:23 PM
RE: Cold Expansion Joint - eaadams - 08-14-2011, 09:50 PM
RE: Cold Expansion Joint - CC Solutions - 08-15-2011, 04:04 AM
RE: Cold Expansion Joint - Ernesto - 08-16-2011, 08:11 PM
RE: Cold Expansion Joint - CC Solutions - 08-19-2011, 07:14 AM
RE: Cold Expansion Joint - eaadams - 10-21-2011, 06:53 PM
RE: Cold Expansion Joint - CC Solutions - 10-21-2011, 07:30 PM
RE: Cold Expansion Joint - eaadams - 10-21-2011, 07:49 PM
RE: Cold Expansion Joint - CC Solutions - 10-22-2011, 07:24 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post

Users browsing this thread:
2 Guest(s)