We are doing some construction with some potential moisture issues in some slabs and some folks recommended using some moisture control sealants to solve the problem prior to finished floors.

The sub recommended either Koester or Synthetics International.
Anyone have any experience with these manufacturers.

Thanks
Drew

06-01-2011, 12:44 AM #2
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Drew,

Where are you? Be careful of subs who recommend moisture products because those two products are not equal. In my opinion, they are at different levels.

Adam @ Synthetics is one of the best salesmen I've ever met. His sales software is amazing, he can track and follow up amazingly well - I could learn a lot from him. But I can tell you that I've passed on some major projects with Synthetics on the concrete. He has a broad spectrum of product. They aren't all the same. And as a flooring distributor I've had to really put the hammer down on subs who don't know the difference.

For me, Koester is the gold standard here in my part of California. When the entire floor comes up, and the hospital shuts down, and everyone lawyers up, and then the lawyers consultant up, the consultants always write the spec along the lines of:
Koester VAP 1 2000 or Ardex MC1 or Mapei EMB or equal.

"Or Equal" - a phrase I HATE in architecture. Nothing is really equal but I believe what you need to look at carefully is the Perm rating.

In my area the Koester rep is the expert. He's really been a beacon for me on doing things right or not at all. He continues to teach me a lot. When we have a problem I turn to him immediately.

I've never had a failure over properly done Koester.

And you don't have to take my word for it. Look at who's logo is on this document. They are the scientists for the Portland Cement Association and you do what they say period, the ultimate consultants. http://www.koesterusa.com/Testing/ASTM-E96-Results-for-VAP-I-2000-andVAP-I-2000FS.pdf

06-07-2011, 08:09 AM #3
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Yes I have experience with Koester. As Eaadams said, it's in the gold standard classification.

Please clarify your issues and I know we can help you out here.... Smile

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

06-07-2011, 10:37 AM #4
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
Have had experience with Koester and Ardex. Both are good products. the key is to do the prep correctly and apply the product to Mfg specification.
Regards
Rayt

06-07-2011, 12:45 PM #5
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Oops, I should say I'm a certified applicator of Koester and Ardex, and one of the first Nora Mitigation applicators in the US. (yea! nora!!! )
And Ray is 110% correct that prep is the most important part of any project. I am on every job my company does and I certify every part of each step. I go as far as using stop watches to time mixing and laying the ICRI molds on every floor to verify CSP profiles. It is routine for my guys now and it doesn't take much time to guarantee it's done by the book.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

06-07-2011, 01:00 PM #6
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
JD
The industry needs more people with your dedication!
Rayt

06-07-2011, 01:15 PM #7
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
You know my background Ray, lifetime warranty with no excuses. It was always in the prep or the installation so let's check things out then double check, and then follow the directions....
Then if it goes wrong, at least my rear is covered as well as it can be... Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

06-08-2011, 08:53 PM #8
MAD123 Unregistered
 
Spam has been removed. -admin

06-09-2011, 06:09 AM #9
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Spam has been removed. love your comment JD. -admin


[/quote]

I completely agree with your statement about the tree chasing the house, but I don't think the fish hook square box ladder thing is correct.... Perhaps Eaadams or Stephen can help here.....

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 8,607 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
4 Replies 11,243 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 28,241 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 7,348 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
9 Replies 39,902 Views
Last Post by eaadams
11-08-2013, 01:41 PM
2 Replies 10,093 Views
Last Post by eaadams
09-27-2013, 10:26 AM
35 Replies 100,912 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 14,464 Views
Last Post by eaadams
01-30-2013, 04:43 PM
4 Replies 15,153 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
32 Replies 92,155 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM

Users browsing this thread:
1 Guest(s)