  • 0 Vote(s) - 0 Average


08-30-2010, 09:53 AM #11
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
(08-25-2010, 05:03 PM)Ernesto Wrote:  Hedenblad, Göran, Drying of Construction Water in Concrete-Drying Times and Moisture Measurement, LT229, Swedish
Council for Building Research, Stockholm, 1997, 54 pages.

Howard Kanare quotes from this extensively in his AIA presentation. Also shows from the same school, a computer program that while in Sweedish that helps with concrete dry times and mix designs.

I believe that Kanare holds the patents for RapidRH








Messages In This Thread
Certified Testing Results - Wesley Holley - 10-30-2008, 10:52 PM
RE: Certified Testing Results - Ernesto - 09-21-2009, 04:20 PM
RE: Certified Testing Results - fyifloors - 08-11-2010, 12:58 AM
RE: Certified Testing Results - Ernesto - 08-22-2010, 09:44 PM
RE: Certified Testing Results - fyifloors - 08-22-2010, 09:52 PM
RE: Certified Testing Results - Ernesto - 08-23-2010, 08:47 AM
RE: Certified Testing Results - fyifloors - 08-23-2010, 01:48 PM
RE: Certified Testing Results - Ernesto - 08-23-2010, 04:52 PM
RE: Certified Testing Results - fyifloors - 08-24-2010, 04:27 PM
RE: Certified Testing Results - Ernesto - 08-25-2010, 05:03 PM
RE: Certified Testing Results - eaadams - 08-30-2010, 09:53 AM
RE: Certified Testing Results - CC Solutions - 09-20-2010, 03:01 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 12,291 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
2 Replies 10,747 Views
Last Post by eaadams
09-27-2013, 10:26 AM
33 Replies 85,208 Views
Last Post by eaadams
11-21-2012, 10:19 AM
51 Replies 143,405 Views
Last Post by ILLENTINC
11-19-2012, 11:59 AM
4 Replies 16,086 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
22 Replies 56,617 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
4 Replies 15,645 Views
Last Post by CC Solutions
10-13-2011, 03:09 PM
36 Replies 104,800 Views
Last Post by CC Solutions
04-19-2011, 04:59 PM
9 Replies 31,766 Views
Last Post by CC Solutions
04-05-2011, 05:33 AM

Users browsing this thread:
1 Guest(s)