Just had a testing firm do a slab for us.

CaCl went from 3.7-4.7
rH went from 95.3-99.4 (not rapidrh probes, unfortunately)

yikes!

But what was interesting and relevant to a thread is that the testing firm did a QC test site which I take to mean Quality Check. At one test site they did two rH tests (not on the report but in the picture) and they did two CaCl tests. The CaCl tests came out the same. But I am not sure showing two tests next to each other is necessarily a valid gauge of quality.

Does anyone know if this quality check type test is in the ASTM literature?








Messages In This Thread
Interesting Test Result - eaadams - 05-03-2011, 09:31 AM
RE: Interesting Test Result - Ernesto - 05-03-2011, 03:46 PM
RE: Interesting Test Result - eaadams - 05-03-2011, 04:21 PM
RE: Interesting Test Result - CC Solutions - 05-04-2011, 10:15 AM
RE: Interesting Test Result - eaadams - 05-06-2011, 11:42 AM
RE: Interesting Test Result - CC Solutions - 05-06-2011, 12:26 PM
RE: Interesting Test Result - Ernesto - 05-06-2011, 04:33 PM
RE: Interesting Test Result - CC Solutions - 05-06-2011, 04:41 PM
RE: Interesting Test Result - Ernesto - 05-06-2011, 05:29 PM
RE: Interesting Test Result - eaadams - 05-07-2011, 03:08 AM
RE: Interesting Test Result - CC Solutions - 05-07-2011, 06:08 AM
RE: Interesting Test Result - Ernesto - 05-07-2011, 05:41 PM
RE: Interesting Test Result - CC Solutions - 05-07-2011, 05:47 PM
RE: Interesting Test Result - mwoody - 08-08-2011, 07:50 AM
RE: Interesting Test Result - CC Solutions - 08-08-2011, 09:03 AM
RE: Interesting Test Result - mwoody - 08-08-2011, 09:45 AM
RE: Interesting Test Result - CC Solutions - 08-08-2011, 11:41 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
6 Replies 18,368 Views
Last Post by Ernesto
05-13-2013, 04:51 PM
10 Replies 30,649 Views
Last Post by eaadams
01-18-2013, 04:48 PM
3 Replies 16,616 Views
Last Post by Ernesto
08-30-2010, 12:42 PM
5 Replies 20,609 Views
Last Post by Ernesto
07-12-2010, 07:00 PM
2 Replies 12,842 Views
Last Post by eaadams
07-09-2010, 09:45 AM
14 Replies 52,260 Views
Last Post by CC Solutions
01-15-2010, 09:36 PM
2 Replies 13,478 Views
Last Post by CC Solutions
12-16-2009, 11:45 AM
3 Replies 17,571 Views
Last Post by rthompson
11-04-2008, 10:03 AM

Users browsing this thread:
1 Guest(s)